🏗️ Civil Engineering

8.2 Ingredients of Concrete

Start MCQ Practice →

8.2 Ingredients of Concrete

Subject: Civil Engineering Chapter: Concrete Technology Topic: 8.2 Ingredients of Concrete

1. Introduction

Concrete is made by mixing four basic ingredients, namely cement, fine aggregate, coarse aggregate and water, together with admixtures when special properties are required. The quality of concrete depends directly on the quality of its ingredients, because the strength and durability of the final product can never exceed the quality of the weakest constituent. For a civil engineering candidate, a detailed knowledge of each ingredient, its types, its desirable properties and the requirements of the relevant Indian Standard codes is essential, because questions on the ingredients of concrete appear regularly in competitive examinations.

Cement is the binding material that reacts with water to form a cement paste, which fills the spaces between the aggregates and binds them together into a solid mass. The aggregates occupy about 60 to 80 percent of the total volume of concrete and provide the bulk and the structural skeleton, while the cement paste fills the voids and provides the adhesive strength. Water, besides making the mix workable, takes part in the chemical reaction of hydration with the cement and controls the strength and durability of the concrete.

In this chapter we will study each ingredient of concrete in detail, starting with the types and composition of cement, then the requirements of fine and coarse aggregates, then the role of water, and finally the function of admixtures. The properties required by the Indian Standard codes, such as IS 456, IS 383 and IS 269, will be emphasised because code values are frequently asked in objective examinations.

2. Cement

Cement is a finely ground inorganic material which, when mixed with water, forms a paste that sets and hardens by hydration. The most common type is ordinary Portland cement, whose name comes from its similarity to the stone from the island of Portland in England. The raw materials for Portland cement are calcareous materials such as limestone or chalk, which supply the lime, and argillaceous materials such as clay or shale, which supply the silica, alumina and iron oxide. The dry process or the wet process is used to grind and mix these materials, and the raw mix is then heated in a rotary kiln to a temperature of about 1400 to 1500 degrees Celsius to form clinker.

The clinker is cooled and ground with a small amount of gypsum to produce the finished cement. The principal compounds of Portland cement are tricalcium silicate (C3S), dicalcium silicate (C2S), tricalcium aluminate (C3A) and tetracalcium aluminoferrite (C4AF). The C3S hydrates quickly and contributes to the early strength, the C2S hydrates slowly and contributes to the later strength, the C3A reacts rapidly with water and is responsible for the flash set which the gypsum is added to control, and the C4AF contributes little to strength but affects the colour and the heat of hydration. The standard grade of OPC used in general construction is 53 grade, whose minimum compressive strength is 53 MPa at 28 days, with 43 grade and 33 grade also available for less demanding work.

Different types of cement are manufactured for different purposes. Portland pozzolana cement contains pozzolanic materials such as fly ash, which improves the durability and reduces the heat of hydration, making it suitable for mass concrete. Rapid hardening cement attains strength more quickly by having a higher C3S content, slag cement contains ground granulated blast furnace slag and is used in marine and aggressive environments, and low heat cement is specially made for mass concrete structures where the heat of hydration must be limited. The soundness of cement, which is its ability to retain its volume after setting without expansion, is tested by the Le Chatelier apparatus and the autoclave test.

3. Aggregates

Aggregates are the inert granular materials, such as sand, gravel and crushed stone, that are mixed with cement and water to form concrete. The fine aggregate is the material passing through a 4.75 mm sieve, and it is usually natural river sand, crushed stone sand or a combination of the two. The coarse aggregate is the material retained on a 4.75 mm sieve, and it is normally crushed stone or gravel of maximum size between 20 mm and 40 mm for general reinforced concrete work. Aggregates should be hard, durable, strong, clean and free from organic impurities, silt and clay, because these impurities interfere with the bond between the paste and the aggregate.

The particle size distribution of the aggregates is called grading, and a well-graded aggregate contains particles of various sizes so that the smaller particles fill the voids between the larger ones. Well-graded aggregates give a dense concrete with a lower cement requirement, while poorly graded aggregates leave voids that must be filled with additional paste. The fineness modulus is a numerical index of the fineness of the aggregate, obtained by dividing the sum of the cumulative percentages retained on the standard sieves by 100, and the usual range of the fineness modulus for fine aggregate is 2.2 to 3.2. The surface texture and the shape of the aggregate particles, whether rounded, angular, flaky or elongated, also affect the workability and the bond strength of the concrete.

The bulking of sand is an important property of fine aggregate; the volume of moist sand is larger than the volume of the same sand when dry, because the moisture forms films around the particles and pushes them apart. Since sand is measured by volume in field batching, allowance must be made for bulking, otherwise the concrete will be short of sand. The bulking of sand increases with moisture content up to about 5 percent, at which point the bulking is maximum, and it decreases again as the sand approaches saturation. The grading zones of fine aggregate specified in IS 383 are zones I to IV, with zone I being the coarsest and zone IV the finest.

4. Water and Admixtures

Water is the ingredient that starts the chemical reaction of hydration and makes the concrete workable. Potable water is generally suitable for mixing concrete, and the water should be clean and free from harmful amounts of oil, acids, alkalis, salts and organic matter. Seawater should not be used for reinforced concrete because the chlorides present in it corrode the steel reinforcement, although it may sometimes be tolerated in plain unreinforced concrete. The quantity of water must be controlled carefully because the water-cement ratio governs the strength, durability and workability of the concrete, and an excess of water creates voids which reduce the strength.

The water-cement ratio is the ratio of the weight of water to the weight of cement in the mix, and for a well-compacted concrete its value lies typically between 0.4 and 0.6. A higher water-cement ratio makes the concrete more workable but weaker, while a lower ratio gives stronger and more durable concrete that is harder to place. The maximum water-cement ratios for different exposure conditions are specified in IS 456 to ensure durability; for example, mild exposure permits a maximum of 0.55 while severe exposure requires not more than 0.45.

Admixtures are materials added to the concrete mix in small quantities, usually less than 2 percent by weight of cement, to modify the properties of the fresh or hardened concrete. Plasticizers and superplasticizers are water-reducing admixtures that improve the workability without adding water, so that a concrete of high workability can be made with a low water-cement ratio. Retarders delay the setting time and are useful in hot weather concreting, accelerators shorten the setting time and are useful in cold weather or for quick repair work, air-entraining agents entrain microscopic air bubbles to improve the resistance to freezing and thawing, and pozzolanic admixtures such as fly ash and silica fume improve the durability and the later strength of the concrete.

5. Quick Revision Tables

Table 1: Principal Compounds of Portland Cement

Compound Short form Proportion (approx.) Contribution
Tricalcium silicate C3S 40-50 percent Early strength
Dicalcium silicate C2S 25-35 percent Later strength
Tricalcium aluminate C3A 8-14 percent Flash set, heat of hydration
Tetracalcium aluminoferrite C4AF 8-12 percent Colour, minor strength

Table 2: Types of Cement and Their Uses

Type of cement Special feature Main use
Ordinary Portland cement General purpose All general construction
Rapid hardening cement High C3S, faster strength Quick repair, cold weather
Portland pozzolana cement Fly ash added Mass concrete, durable structures
Slag cement Blast furnace slag Marine and aggressive exposure
Low heat cement Low heat of hydration Large mass concrete dams
White cement No iron oxide Architectural and decorative work

6. Mind Map

flowchart TD
    A[Ingredients of Concrete] --> B[Cement]
    A --> C[Fine aggregate]
    A --> D[Coarse aggregate]
    A --> E[Water]
    A --> F[Admixtures]
    B --> B1[C3S early strength]
    B --> B2[C2S later strength]
    B --> B3[C3A flash set]
    B --> B4[Gypsum controls setting]
    C --> C1[Sand passing 4.75 mm]
    C --> C2[Bulking of sand]
    D --> D1[20-40 mm crushed stone]
    D --> D2[Grading and fineness modulus]
    E --> E1[Hydration]
    E --> E2[Water-cement ratio]
    F --> F1[Plasticizers and superplasticizers]
    F --> F2[Retarders and accelerators]
    F --> F3[Air-entraining agents]
    A --> G[IS 383 grading zones]

7. Important Diagrams (SVG)

The following diagrams show the composition of concrete in terms of its ingredients and the hydration reaction of cement with water.

Composition of a Typical Concrete Mix Cement paste Cement + Water + Air about 30% Fine aggregate about 25% Coarse aggregate about 45% Aggregates occupy 60 to 80 percent of the total volume Cement paste fills the voids and binds the aggregates Golden Rule Well-graded aggregates reduce the voids so less cement paste is needed.

Hydration Reaction and Setting of Cement CEMENT C3S, C2S, C3A WATER H2O Mixing HYDRATION C-S-H GEL strength giving compound HEAT + LIME released during reaction Initial setting time of OPC: not less than 30 minutes Final setting time of OPC: not more than 600 minutes Gypsum is added to clinker to control the rapid reaction of C3A Golden Rule Cement gains strength by hydration; gypsum prevents flash set of C3A.

8. Common Mistakes

  1. Many students believe that all the water added to concrete takes part in hydration, but most of it only makes the mix workable and later evaporates, leaving pores.
  2. A frequent error is to use seawater for reinforced concrete, which causes corrosion of the steel reinforcement through the chloride content.
  3. Some candidates confuse the terms fine aggregate and coarse aggregate; the dividing sieve size is 4.75 mm.
  4. Students often forget the phenomenon of bulking of sand, which increases the volume of moist sand and leads to a sand shortage if not allowed for in volume batching.
  5. A common mistake is to think that more cement always gives stronger concrete; beyond the optimum content, extra cement increases shrinkage and cracking.
  6. Many candidates forget that gypsum is added to the clinker to control the flash set of C3A, and not to increase the strength.
  7. Some students confuse the functions of accelerators, which reduce the setting time, with retarders, which increase it.
  8. Another recurring error is to use aggregate containing organic impurities without washing, which seriously retards the setting of the cement.

9. Exam Tips

  1. Memorise the four main compounds of cement, C3S, C2S, C3A and C4AF, and remember that C3S gives early strength while C2S gives later strength.
  2. Remember the sieve size of 4.75 mm, which separates fine aggregate from coarse aggregate, and the usual maximum aggregate sizes of 20 mm and 40 mm.
  3. Note the fineness modulus range for fine aggregate of 2.2 to 3.2 and the bulking behaviour of sand, which is maximum at about 5 percent moisture.
  4. Know that OPC 53 grade has a minimum 28-day compressive strength of 53 MPa, and that grade numbers increase with the strength.
  5. Remember the maximum water-cement ratios for exposure conditions, such as 0.55 for mild exposure and 0.45 for severe exposure, from IS 456.
  6. Understand the function of each admixture: plasticizers for workability, retarders for hot weather, accelerators for cold weather, and air-entraining agents for frost resistance.
  7. Use the Le Chatelier apparatus for the soundness test of cement and remember that gypsum is added to control the setting.
  8. Recall the grading zones I to IV of IS 383 for fine aggregate, with zone I the coarsest and zone IV the finest.

10. Conclusion

The quality of concrete is decided by the quality of its ingredients, and a civil engineer must therefore understand cement, aggregates, water and admixtures in depth. In this chapter we have studied the manufacture and composition of Portland cement, the role of its principal compounds and the different types of cement available for different applications. We have examined the requirements of fine and coarse aggregates, including their grading, fineness modulus and bulking, and the role of water in hydration and workability. We have also considered the function of admixtures in modifying the properties of concrete for special conditions. The code requirements of IS 456, IS 383 and IS 269, including the maximum water-cement ratios and the standard sieve sizes, have been presented in a form suitable for rapid revision. With this understanding of the ingredients, the candidate is now ready to study the proportioning of these ingredients in the form of mix design and the control of the water-cement ratio, which are the subjects of the following chapters.