8.7 Compaction and Curing

Subject: Civil Engineering Chapter: Concrete Technology Topic: 8.7 Compaction and Curing

1. Introduction

Compaction and curing are the two operations that follow the placing of concrete and decide whether the concrete ever reaches its designed strength. Compaction, also called consolidation, is the process of removing the entrapped air from the fresh concrete so that the concrete becomes dense and the maximum density is achieved, while curing is the process of maintaining the favourable conditions of moisture and temperature so that the hydration of the cement continues and the concrete gains strength. Neither the best ingredients nor the best mix design can compensate for poor compaction or neglected curing, because the entrapped air voids and the dried-out cement paste are permanent sources of weakness.

Freshly placed concrete contains entrapped air in the form of bubbles, which may occupy as much as 5 to 20 percent of the volume of the concrete, and every percent of entrapped air reduces the compressive strength by about 5 to 6 percent. Compaction expels this air by the application of work, either by hand rodding or by mechanical vibration, and a concrete that is compacted to the maximum density is the concrete for which the strength-water cement ratio relationship of Abram's law is valid. A concrete that is left poorly compacted develops honeycombing and surface voids and fails the durability as well as the strength requirements.

In this chapter we will study the need for compaction, the methods of hand compaction and mechanical vibration including the internal, external and surface vibrators, the factors affecting the efficiency of compaction, the importance of curing and the methods of curing, and the duration of curing required for different cements. The standard values such as the frequency of the vibrators, the duration of curing of 7 to 14 days and the effect of air voids on strength are frequently examined.

2. Compaction of Concrete

The compaction of concrete is necessary because the freshly mixed concrete contains entrapped air which, if left in the concrete, creates voids that reduce the strength, increase the permeability and spoil the appearance of the surface. The voids are formed during mixing and placing because the concrete is a mixture of solid particles with air trapped between them, and compaction removes this air by bringing the particles into close contact. The strength of concrete increases as the degree of compaction increases, until the maximum density is reached, and the concrete that is compacted to the maximum density has the strength predicted by the water-cement ratio.

The compaction can be done by hand or by mechanical means. Hand compaction is done by rodding, by tamping and by spading, and it is used only for small quantities of work and for concrete of high workability. Rodding is done with a tamping rod of 16 mm diameter, which is pushed into the concrete to drive out the air, tamping is done by striking the surface of the concrete with a flat tool, and spading is done by working a spade or a similar tool along the formwork to remove the air trapped against the forms. Hand compaction is slow, and it cannot compact stiff mixes, so mechanical compaction is used for almost all important works.

Mechanical compaction is done with vibrators, which generate high-frequency vibrations that fluidise the concrete momentarily and cause the entrapped air to rise to the surface. The internal vibrator, also called the needle vibrator or poker, is the most common type, and it consists of a vibrating needle of 25 to 75 mm diameter that is inserted vertically into the concrete and withdrawn slowly after about 2 minutes of vibration. The external vibrator is clamped to the formwork and is used for thin sections and narrow formwork, the table vibrator is used for precast elements, and the surface vibrator or screed is used for slabs and road surfaces. The frequency of the internal vibrator is typically between 3500 and 5000 vibrations per minute.

3. Methods of Curing

Curing is the process of maintaining the concrete in a moist and warm condition during the early stages of hardening, so that the hydration of the cement continues and the concrete gains its full strength. The cement can hydrate only in the presence of water, so if the water in the mix evaporates from the surface, the hydration stops and the surface concrete remains weak, porous and prone to shrinkage cracking. Curing therefore has two purposes: to prevent the loss of moisture from the concrete and to keep the temperature of the concrete within the range favourable for hydration.

The methods of curing are divided into two groups: the methods that supply additional water to the concrete and the methods that prevent the loss of water from the concrete. The water-supplying methods include ponding, in which the surface of the concrete is flooded with water, sprinkling or spray curing, in which water is sprayed on the surface at intervals, wet covering, in which the surface is covered with wet gunny bags or sand, and the use of damp sawdust. These methods are suitable for horizontal surfaces such as slabs, floors and pavements, while ponding is regarded as the most effective method because it keeps the whole surface continuously wet.

The methods that prevent the loss of moisture include the membrane curing and the steam curing. In membrane curing, a water-proof membrane in the form of a curing compound is sprayed on the surface to form a thin film which prevents the escape of moisture, and this method is used for vertical surfaces, columns and where water cannot be supplied easily. Steam curing is used in the precast industry, where the concrete is kept in steam chambers at a temperature of about 90 to 100 degrees Celsius for a few hours, which accelerates the hydration so that the concrete attains in hours the strength that it would take days to develop in normal curing. Hot water or hot air can also be used for accelerated curing.

4. Duration and Significance of Curing

The duration of curing determines the ultimate strength of the concrete. Concrete that is cured for 7 days develops about 65 percent of its 28-day strength, concrete cured for 14 days develops about 90 percent, and concrete cured for 28 days develops the full characteristic strength, while concrete that is not cured at all may develop only about 40 percent of its potential strength. The minimum period of curing recommended for ordinary Portland cement is 7 days, and for concrete with mineral admixtures such as Portland pozzolana cement, the curing period is extended to 10 to 14 days because these cements gain strength more slowly.

The curing is most important in the first few days after placing, because the concrete is most vulnerable to the loss of water during this period and the rate of hydration is highest. The concrete should be kept moist from the time the surface becomes hard enough to resist damage, which is usually after about 24 hours from the placing. In hot weather, the curing must begin earlier and be continued for a longer period because the evaporation is rapid, while in cold weather, the concrete must be protected from freezing because the hydration stops below the freezing point of water.

The effect of the compaction and curing on the strength can be combined into one important observation: the strength of the concrete is governed by the water-cement ratio only when the concrete is fully compacted, and the strength of a fully compacted concrete is developed only by adequate curing. Poor compaction introduces air voids, and poor curing stops the hydration, so both must be done properly together. The quality of the concrete surface, its resistance to abrasion and its impermeability, all depend on the care taken in these two operations.

5. Quick Revision Tables

Table 1: Methods and Duration of Curing

Method Type Best suited for
Ponding Water supplying Slabs, floors, pavements
Sprinkling and spraying Water supplying Columns, walls
Wet covering (gunny bags) Water supplying Horizontal surfaces
Membrane curing compound Moisture retaining Vertical surfaces, tanks
Steam curing Accelerated Precast products
Hot water curing Accelerated Precast and testing

Table 2: Strength Development and Curing Period

Curing period Percentage of 28-day strength
No curing About 40 percent
3 days About 50-55 percent
7 days About 65 percent
14 days About 90 percent
28 days 100 percent (reference)

6. Mind Map

flowchart TD
    A[Compaction and Curing] --> B[Compaction]
    A --> C[Curing]
    B --> B1[Remove entrapped air]
    B --> B2[Hand compaction]
    B --> B3[Mechanical vibration]
    B --> B4[Internal vibrator]
    B --> B5[External vibrator]
    B --> B6[Table and surface vibrators]
    B --> B7[5-6 percent strength loss per percent air]
    C --> C1[Maintain moisture for hydration]
    C --> C2[Ponding]
    C --> C3[Sprinkling]
    C --> C4[Wet covering]
    C --> C5[Membrane curing]
    C --> C6[Steam curing]
    C --> C7[7 days minimum for OPC]
    A --> D[No curing gives only 40 percent strength]

7. Important Diagrams (SVG)

The following diagrams show the use of an internal needle vibrator for compaction and the ponding method of curing concrete.

Compaction by Internal Vibrator FORMWORK with fresh concrete Air bubbles rise to the surface MOTOR Needle vibrator vibrating head Insert needle vertically, withdraw slowly after vibration Needle diameter 25-75 mm, frequency 3500-5000 rpm Vibration stops when mortar appears on the surface Golden Rule Each 1 percent of entrapped air cuts the concrete strength by about 5-6 percent.

Ponding Method of Curing CONCRETE SLAB Sand bund PONDED WATER Kept continuously flooded for 7-14 days Hydration continues as long as moisture is available 7 days curing gives about 65 percent of 28-day strength No curing at all gives only about 40 percent strength Golden Rule Cure OPC concrete for a minimum of 7 days and pozzolana concrete for 14 days.

8. Common Mistakes

  1. Many students think that a little extra air in the concrete is harmless, but each 1 percent of entrapped air reduces the strength by about 5 to 6 percent.
  2. A frequent error is to over-vibrate the concrete, which causes segregation and bleeding instead of improving the quality.
  3. Some candidates use a vibrator to move the concrete sideways in the formwork, which causes segregation; the vibrator should only consolidate the concrete in place.
  4. Students often forget that the internal needle vibrator must be withdrawn slowly and inserted at intervals of about 60 to 75 cm, otherwise the compaction is incomplete.
  5. A common mistake is to stop curing too early; concrete cured for only 3 days develops only about half of the 28-day strength.
  6. Many candidates use steam curing for ordinary site work, forgetting that it is mainly an industrial method for precast products.
  7. Some students think the minimum curing period is 28 days for OPC, whereas the code minimum is 7 days, with 14 days recommended for pozzolana cements.
  8. Another recurring error is to start curing after the concrete has already dried out; curing must begin as soon as the surface is hard enough to resist damage, usually within 24 hours.

9. Exam Tips

  1. Remember the rule of thumb that each 1 percent of entrapped air reduces the compressive strength by about 5 to 6 percent.
  2. Know the types of vibrators: internal or needle, external, table and surface, and the frequency range of 3500 to 5000 rpm for the internal vibrator.
  3. Memorise the strength gain with curing: 7 days about 65 percent, 14 days about 90 percent, and no curing only about 40 percent of the 28-day strength.
  4. Remember the minimum curing period of 7 days for OPC and 10 to 14 days for Portland pozzolana cement.
  5. Note that ponding is the most effective method of curing for horizontal surfaces, while membrane curing is used for vertical surfaces.
  6. Remember that steam curing accelerates the strength gain so that precast concrete develops high early strength in a few hours.
  7. In hot weather, begin curing early and continue longer because the evaporation is rapid, while in cold weather protect the concrete from freezing.
  8. Remember that the strength-water cement ratio relationship is valid only for fully compacted concrete, so compaction is essential for the design to work.

10. Conclusion

Compaction and curing are the two finishing operations that convert the placed concrete into a dense, strong and durable material, and they deserve as much care as the batching and the mixing. In this chapter we have studied the need for compaction to remove the entrapped air, the methods of hand compaction and mechanical vibration with the internal, external, table and surface vibrators, and the effect of the air voids on the strength. We have also studied the purpose of curing in maintaining the moisture for hydration, the methods of curing including ponding, sprinkling, wet covering, membrane curing and steam curing, and the duration of curing required for the different types of cement. The key numerical relationships, such as the 5 to 6 percent loss of strength per percent of air, the 65 percent strength at 7 days and the 90 percent at 14 days, and the minimum curing periods, have been emphasised. The candidate must remember that compaction makes the concrete dense and curing makes the hydration complete, and that both are necessary for the concrete to reach its designed strength and durability.