Subject: Civil Engineering Chapter: Concrete Technology Topic: 8.9 Durability of Concrete
Durability is the ability of concrete to resist weathering action, chemical attack, abrasion and any other process of deterioration, so that it maintains its strength, its appearance and its serviceability throughout the design life of the structure. A durable concrete remains sound and serviceable for many years in the environment in which it is placed, while a non-durable concrete deteriorates through cracking, spalling, corrosion of the reinforcement and loss of strength long before the end of its intended life. The durability of concrete is one of the most important requirements of modern design, because the repair of a deteriorated concrete structure is costly and often difficult, and the Indian Standard IS 456 lays down special requirements for durable concrete.
The durability of concrete is governed primarily by its permeability, which controls the ingress of water, oxygen, carbon dioxide, chlorides and sulphates into the concrete. A dense concrete with a low water-cement ratio and good compaction has low permeability and therefore high durability, while a porous concrete with excess water and poor compaction allows the aggressive agents to penetrate and attack the cement paste and the steel reinforcement. The main factors affecting durability are the water-cement ratio, the cement content, the type of cement, the compaction and the curing, the cover to the reinforcement, and the exposure conditions of the structure.
In this chapter we will study the mechanism of the deterioration of concrete, including the corrosion of reinforcement, the alkali-aggregate reaction, the attack by sulphates and chlorides, the freezing and thawing action and the abrasion, the requirements for durable concrete prescribed by IS 456, and the influence of the exposure conditions on the design. The exposure conditions of mild, moderate, severe, very severe and extreme, and their requirements, are the most frequently tested items in this topic.
The permeability of concrete is the most important single factor controlling its durability, because it determines how easily water and the aggressive chemicals dissolved in the water can enter the concrete. The permeability is controlled by the pores and the micro-cracks in the concrete, which are caused by the excess water, the incomplete compaction and the poor curing. The water-cement ratio is the dominant factor, because a higher water-cement ratio leaves more capillary pores after the excess water evaporates, so the permeability increases rapidly as the water-cement ratio rises above about 0.5.
The cement content and the quality of the paste also affect the permeability. A higher cement content gives a richer paste which fills the voids between the aggregates and reduces the permeability, provided the paste itself is dense. The use of pozzolanic materials such as fly ash and silica fume refines the pore structure and reduces the permeability, which is why such cements are recommended for aggressive environments. The compaction and the curing are equally important, because a fully compacted and well-cured concrete has fewer voids and a denser paste, and the curing must be continued for a sufficient period so that the hydration products fill the pores.
The other factors affecting the durability are the cover to the reinforcement, which protects the steel from the corrosive agents, the maximum size and grading of the aggregates, which influence the porosity, and the presence of cracks, which provide direct channels for the aggressive agents to reach the steel. The durability of concrete therefore requires a combination of a low water-cement ratio, an adequate cement content, good compaction and curing, and an adequate cover, and the code specifies the minimum values of these parameters for each exposure condition.
The corrosion of the steel reinforcement is the most common and the most serious form of deterioration of reinforced concrete, because the corrosion products occupy a much larger volume than the original steel and the resulting expansion cracks and spalls the concrete cover. The steel is normally protected by the alkalinity of the concrete, which maintains a passive film on the surface of the steel, but this protection fails when the chloride ions penetrate to the steel or when the carbonation of the concrete reduces the alkalinity. Carbonation is the reaction of the atmospheric carbon dioxide with the calcium hydroxide of the concrete, which converts the alkaline paste into calcium carbonate and lowers the pH below the value of about 9.5 required to protect the steel.
The alkali-aggregate reaction is a chemical reaction between the alkalis of the cement and the reactive silica of certain aggregates, which forms a gel that absorbs water and expands, causing cracking and map cracking of the concrete surface. The alkali-silica reaction is the most common form, and it is controlled by using non-reactive aggregates, by limiting the alkali content of the cement, and by adding pozzolanic materials which consume the alkalis. The sulphate attack occurs when the sulphates in the soil or the groundwater react with the tricalcium aluminate of the cement to form ettringite, which expands and cracks the concrete, and it is resisted by using sulphate-resisting cement with a low C3A content.
The freezing and thawing action destroys the concrete when the water in the pores freezes and expands, and the repeated cycles of freezing and thawing progressively crack the surface and cause scaling, which is resisted by air-entrained concrete with microscopic air bubbles that accommodate the expansion. The abrasion and erosion of the concrete surface by the movement of traffic, water and particles reduce the thickness of the cover and expose the aggregates, and the concrete for such surfaces is made with hard aggregates and a low water-cement ratio. The fire resistance, chemical attack by acids and the attack by seawater, which involves both the chloride and the sulphate actions, are the other forms of deterioration that must be considered in the design.
IS 456 classifies the environment of the structure into five exposure conditions, namely mild, moderate, severe, very severe and extreme, depending on the degree of aggressiveness of the surroundings. For each exposure condition, the code prescribes the maximum water-cement ratio, the minimum grade of concrete and the minimum cement content, and the minimum nominal cover to the reinforcement. For example, mild exposure permits concrete of grade M20 with a maximum water-cement ratio of 0.55, while severe exposure requires concrete of grade M30 with a maximum water-cement ratio of 0.45, and extreme exposure requires grade M40 with a maximum water-cement ratio of 0.40.
The minimum cement content prescribed for the exposure conditions ensures that the paste is rich enough to produce a dense and impermeable concrete. The nominal cover, which is the distance from the surface of the reinforcement to the outer surface of the concrete, must be sufficient to protect the steel from the corrosive agents and to provide the required fire resistance. The minimum nominal cover for the general requirements is 25 mm for mild exposure and 45 mm for moderate exposure in the case of beams and columns, and these values increase for the severe and extreme exposures.
The requirements for durable concrete also include the use of suitable materials, such as the sulphate-resisting cement in the sulphate-bearing soils, the air-entrained concrete in the cold climates, and the proper admixtures for reducing the water demand and improving the workability. The concrete must be compacted fully and cured properly, and the cracks must be limited so that the width of the cracks does not exceed the limits specified in the code, which depend on the exposure condition. The durability of concrete is thus achieved not by a single measure but by the combination of the correct mix, the correct cover, the correct construction practices and the correct protection.
| Exposure | Max water-cement ratio | Min grade | Min cement content (kg/m3) |
|---|---|---|---|
| Mild | 0.55 | M20 | 300 |
| Moderate | 0.50 | M25 | 300 |
| Severe | 0.45 | M30 | 320 |
| Very severe | 0.45 | M35 | 340 |
| Extreme | 0.40 | M40 | 360 |
| Deterioration type | Cause | Prevention |
|---|---|---|
| Corrosion of steel | Chlorides, carbonation | Adequate cover, low permeability |
| Carbonation | CO2 from air | Dense concrete, good curing |
| Sulphate attack | Sulphates in soil and water | Sulphate-resisting cement |
| Alkali-aggregate reaction | Reactive silica + alkalis | Non-reactive aggregate, low alkali cement |
| Freezing and thawing | Freezing of pore water | Air entrainment |
| Abrasion | Traffic, water erosion | Hard aggregate, low water-cement ratio |
flowchart TD
A[Durability of Concrete] --> B[Permeability]
A --> C[Corrosion of steel]
A --> D[Carbonation]
A --> E[Sulphate attack]
A --> F[Alkali-aggregate reaction]
A --> G[Freezing and thawing]
A --> H[Exposure conditions]
B --> B1[Water-cement ratio]
B --> B2[Compaction and curing]
B --> B3[Cement content and pozzolana]
C --> C1[Passive film destroyed]
C --> C2[Expansion and spalling]
H --> H1[Mild 0.55 M20]
H --> H2[Moderate 0.50 M25]
H --> H3[Severe 0.45 M30]
H --> H4[Very severe 0.45 M35]
H --> H5[Extreme 0.40 M40]
A --> I[Cover to reinforcement]
A --> J[Requirements of IS 456]
The following diagrams show the corrosion of reinforcement due to the ingress of chlorides and the mechanism of the alkali-aggregate reaction.
The durability of concrete determines the length of the useful life of a structure, and it must be designed into the concrete from the very beginning through the choice of the mix, the cover and the construction practices. In this chapter we have studied the factors controlling the durability, particularly the permeability, the mechanisms of the deterioration of concrete including the corrosion of steel, carbonation, the sulphate attack, the alkali-aggregate reaction, the freezing and thawing and the abrasion, and the requirements of IS 456 for durable concrete under the five exposure conditions. The exposure conditions of mild, moderate, severe, very severe and extreme, and the corresponding maximum water-cement ratios, minimum grades and minimum cement contents, have been presented in tabular form for rapid revision. The candidate must remember that the durability is achieved by the combination of a low water-cement ratio, an adequate cement content, good compaction and curing, an adequate cover, and the correct choice of the materials for the environment. With this understanding of durability, the candidate is now ready to study the special concretes, which extend the range of the concrete technology into the special applications.