🏗️ Civil Engineering

7.8 Damp Proofing and Waterproofing

Start MCQ Practice →

7.8 Damp Proofing and Waterproofing

Subject: Civil Engineering Chapter: Building Construction Topic: 7.8 Damp Proofing and Waterproofing

1. Introduction

Dampness is one of the most persistent and damaging problems of buildings. Moisture enters a building from the ground by capillary rise, from the walls through rain, from the roof through leaks, and from the atmosphere through condensation, and it gradually destroys the structure, spoils the finishes and endangers the health of the occupants. Dampness in walls causes efflorescence, the whitish crystalline deposit on the surface, the softening and disintegration of plaster, the decay of timber, the corrosion of steel and the growth of fungus and mould. For these reasons damp proofing and waterproofing are among the most important operations in building construction, and the sources of dampness, the methods of prevention and the materials used form a favourite topic for competitive examinations such as SSC JE, RRB JE and state AE/JE papers.

The term damp proofing usually refers to the prevention of moisture entering a building through walls and floors by the capillary action of the ground, while waterproofing refers to the treatment of the roof, tanks, basements and other surfaces which remain in contact with water or rain. A damp proof course, abbreviated as DPC, is a layer of impervious material provided at the plinth level and other critical levels of the building to stop the rise of moisture. The DPC may be made of a rigid material such as cement concrete, or a semi-rigid material such as bitumen, or a flexible material such as bitumen felt, and its position and construction follow well-established rules.

In this chapter we will study the sources of dampness in buildings, the ill effects of dampness, and the principles of damp proofing. We will learn the types of damp proofing materials, the position at which a damp proof course is laid, and the methods of providing it in walls, floors and roofs. We will also study the special waterproofing of basements, water tanks, terraces and bathrooms, because the examiner tests the application of waterproofing techniques to these specific situations.

2. Sources and Ill Effects of Dampness

Dampness in a building can arise from four principal sources. The first and most common source is the moisture of the ground, which rises through the porous materials of the foundation and the wall by capillary action and appears on the wall face at and above the plinth level. The second source is rain, which enters through the roof, the parapet, the junction of the roof with the wall, the chajjas, the window sills and the door thresholds. The third source is the water that is used in the building, such as the water of bathrooms, kitchens, sinks and washing places, which seeps through the floors and walls if they are not made impervious. The fourth source is atmospheric moisture, which condenses on the cold inner surfaces of walls and roofs, especially in winter.

The ill effects of dampness are numerous and serious. Damp walls lose their strength and durability, the plaster softens, blisters and peels, and the paint flakes away. Efflorescence appears on the face of the walls as a white deposit of soluble salts. Dampness causes the corrosion of the reinforcement of RCC members, which expands and cracks the concrete, the decay and warping of timber, and the rusting of steel doors, windows and fittings. It promotes the growth of termites, fungus and mould, which destroy wood and produce a musty smell. Dampness also spoils the internal furnishings, reduces the thermal comfort of the building because damp materials conduct heat and cold more readily, and is dangerous to health because it produces an unhealthy atmosphere for the occupants.

The principles of damp proofing follow directly from these sources. Dampness must be prevented by stopping the rise of moisture from the ground by a damp proof course, by protecting the walls from rain through proper roof overhangs, chajjas and copings, by making the floors and walls of wet areas impervious, and by ventilating the building to reduce condensation. A building is made damp proof by providing a continuous and impervious layer, the damp proof course, at the critical sections, so that no capillary path remains for the moisture to travel.

3. Damp Proofing Materials and Methods

The materials used for damp proofing are classified as rigid, semi-rigid and flexible. The rigid materials include cement concrete of 1:1.5:3 mix with a waterproofing compound, and stone, which are strong and durable but crack under movement. The semi-rigid materials include bitumen, mastic asphalt and bituminous mixtures, which can accommodate slight movement. The flexible materials include bitumen felt, synthetic rubber sheets, polythene and aluminium foils, which are laid as membranes and are not affected by movement or vibration. A good damp proofing material must be impervious, strong and durable, not affected by the salts in the soil, easy to lay, and economical.

The most common DPC used in buildings is cement concrete of 1:1.5:3 mix with a waterproofing compound, laid to a thickness of about 2.5 cm to 5 cm. It is placed in the wall at the plinth level, just above the ground level, so that the rising ground moisture is stopped. The DPC should be laid on a level bed, projecting on both faces of the wall by about 2 cm, and a vertical DPC is also provided in the external walls of the foundation where required. The DPC should be continuous across the whole wall, and its joints should be lapped and sealed, because a break in the DPC forms a path for the moisture. The DPC should not be exposed on the outside face in wet areas, and it should be covered by the plaster.

For roofs, the water-proofing is provided by the brick bat coba, the lime concrete and the bitumen felt treatments already described in the chapter on roofs, and by the modern synthetic membranes. For basements, the water-proofing is provided on the outer face of the walls and under the floor slab, because the pressure of the ground water is active and the treatment must resist water under pressure. For water tanks, the interior is plastered with a rich cement mortar mixed with a waterproofing compound, or a flexible membrane is applied. For bathrooms and wet areas, the floor and the lower part of the walls are made water-proof by a layer of cement mortar with a waterproofing compound or a sheet membrane, and the junctions are made watertight.

4. Position of the Damp Proof Course and Special Treatments

The damp proof course is provided at several levels in a building, and its position is decided by the source of moisture. The most important position is the plinth level, where the DPC stops the rise of moisture from the ground into the walls; it should be placed at least 15 cm above the ground level and about 30 cm above the finished floor level. A DPC is also provided at the base of the external walls below the coping, at the sills and lintels of windows, at the top of parapet walls, and under the roof slab. In the case of heavy rainfall or a high water table, the DPC of the wall is combined with a vertical DPC on the outer face of the external walls and a horizontal DPC under the floor.

The ground floor of a building is made damp proof by the damp proof course laid over the base course and below the floor finish. The concrete DPC under the floor should be at least 10 cm to 15 cm thick, and where the water table is high, a flexible membrane such as bitumen felt or polythene is laid under the floor slab to resist the hydrostatic pressure. The cavity walls are provided with a DPC at the base and at the top of the cavity, and the wall ties are provided so that moisture does not cross the cavity. In a building with a basement, the entire basement is treated as a tank, with the water-proofing membrane carried continuously over the floor and the walls to the top of the basement, because any break at the junction causes leakage.

The treatment of roofs and terraces requires the surface to be prepared first. The roof slab is cleaned, dried and made free from dust, and all cracks are cut and filled with the water-proofing compound. The bitumen felt is then laid in layers, each layer lapping over the previous one, and the joints are sealed with heat. The brick bat coba is laid to a slope towards the rain water outlets, and the surface is finished with a cement mortar screed with a slope of about 1 in 50. The parapet is waterproofed at the junction with the roof by a moulded cove, and the top of the parapet is capped with a coping stone or a weather-proof finish. The success of the treatment depends on the care of the workmanship and the continuity of the membrane.

5. Quick Revision Tables

Table 1: Sources of Dampness and Remedies

Source of dampness How moisture enters Remedy
Ground moisture Capillary rise through walls DPC at plinth level
Rain Roof, parapet, chajja, sills Water-proof roof, overhangs, copings
Internal water Bathroom, kitchen seepage Impervious floors, membranes
Condensation Cold internal surfaces Ventilation and insulation

Table 2: Damp Proofing Materials by Type

Type Materials Properties
Rigid Cement concrete 1:1.5:3, stone Strong, cracks under movement
Semi-rigid Bitumen, mastic asphalt Tolerates slight movement
Flexible Bitumen felt, polythene, rubber Not affected by movement
Integral Water-proofing compounds in mortar Waterproof mortar internally

6. Mind Map

flowchart TD
    A[Damp Proofing and Waterproofing] --> B[Sources of dampness]
    A --> C[Ill effects]
    A --> D[Damp proofing materials]
    A --> E[Position of DPC]
    A --> F[Special treatments]
    B --> B1[Ground moisture - capillary rise]
    B --> B2[Rain - roof, sills]
    B --> B3[Internal water]
    B --> B4[Condensation]
    C --> C1[Efflorescence]
    C --> C2[Corrosion of steel]
    C --> C3[Decay of timber]
    C --> C4[Fungal growth]
    D --> D1[Rigid concrete]
    D --> D2[Bitumen felt]
    D --> D3[Polythene membranes]
    E --> E1[At plinth level]
    E --> E2[Under floor]
    E --> E3[At sills and lintels]
    F --> F1[Basement tanking]
    F --> F2[Roof water-proofing]
    F --> F3[Water tank lining]

7. Important Diagrams (SVG)

The following diagrams show the position of the damp proof course in a wall and the method of water-proofing a roof.

Position of Damp Proof Course WALL DPC Floor finish Ground level 15 cm above ground Arrows show moisture rising Capillary rise is stopped by the DPC at plinth level. Golden Rule Provide the DPC at plinth level, 15 cm above ground, continuous across the wall.

Water-proofing of a Flat Roof RCC roof slab Bitumen felt membrane (2 to 3 layers) Cement mortar screed with slope 1 in 50 Pipe Rain water flows towards the outlet pipe Direction of slope Junction of roof and parapet sealed with a moulded cove. Golden Rule The roof is waterproofed by a continuous membrane sealed at all joints and slopes.

8. Common Mistakes

  1. Many students think that a DPC is needed only in the walls; a DPC is also required under the floor and at the sills, lintels and parapets.
  2. A common error is to place the DPC below the ground level; it should be placed at least 15 cm above the ground so that rain splash does not carry moisture over it.
  3. Some candidates believe that cement mortar alone is waterproof; an ordinary mortar is porous and requires a waterproofing compound or a membrane.
  4. Students frequently forget that the DPC must be continuous; a break or a badly lapped joint in the DPC is the most common cause of local dampness.
  5. A frequent mistake is to treat the roof slab as naturally waterproof; the RCC slab is porous and develops shrinkage and temperature cracks that must be sealed.
  6. Many candidates ignore the pressure of ground water in basements; the water-proofing must be carried continuously over floor and walls like a tank.
  7. Another common error is to finish a terrace level; the water-proofing screed must slope about 1 in 50 towards the outlets.
  8. Students often forget the moulded cove at the roof and parapet junction; it is precisely at this junction that most terrace leakages occur.

9. Exam Tips

  1. Remember the position of the DPC: at plinth level, at least 15 cm above the ground and about 30 cm above the finished floor.
  2. Memorise the types of DPC materials: rigid concrete 1:1.5:3 with waterproofing compound, semi-rigid bitumen, and flexible bitumen felt and polythene.
  3. Learn the sources of dampness in order: capillary rise from ground, rain penetration, internal water and condensation.
  4. Recall that efflorescence is the white deposit of soluble salts on damp walls, a direct one-mark favourite.
  5. Note that basements are waterproofed like a tank, with the membrane continuous over floor and walls to resist ground water pressure.
  6. Remember that a bathroom floor must slope towards the drain and be finished with an impervious waterproofing membrane.
  7. Practise one-line answers on the ill effects: corrosion of reinforcement, decay of timber, flaking of paint, growth of fungus.
  8. Revise the roof water-proofing sequence: clean and dry the slab, fill cracks, lay bitumen felt with laps, seal joints, screed with slope 1 in 50.

10. Conclusion

Dampness is the quiet enemy of every building, and its prevention through damp proofing and waterproofing is essential for the strength, durability, comfort and health of a structure. In this chapter we have studied the four sources of dampness, namely the capillary rise of ground moisture, the penetration of rain, the water used inside the building and atmospheric condensation, and the serious ill effects such as efflorescence, corrosion, decay and fungal growth. We have learned the materials of damp proofing, from rigid concrete and semi-rigid bitumen to flexible membranes, and the position of the DPC at the plinth, under floors and at sills, lintels and parapets. We have also studied the special treatments for roofs, basements, water tanks and bathrooms, which require continuous membranes, proper slopes and sealed junctions. A candidate who remembers the position and continuity of the DPC, the classification of materials and the special cases will answer the damp proofing and waterproofing questions of the building construction paper with confidence.