🏗️ Civil Engineering

6.1 Bricks

Start MCQ Practice →

6.1 Bricks

Subject: Civil Engineering Chapter: Building Materials Topic: 6.1 Bricks

1. Introduction

Bricks are the most ancient and the most widely used building material in the world, and in India they remain the backbone of masonry construction for walls, foundations, arches and pavements. A brick is a small rectangular building unit made from clay, moulded to size and then hardened by drying and burning. Because clay is available in abundance almost everywhere, bricks are cheap, durable and easily manufactured, which is why they dominate residential and low-rise construction in the country. For a candidate preparing for civil engineering examinations such as SSC JE, RRB JE and State AE exams, the chapter on bricks is a very high-yield topic, and direct one-mark questions on brick sizes, classification, tests and manufacturing defects appear year after year.

The quality of a brick depends primarily on the quality of the clay used and the care taken during moulding, drying and burning. Good brick clay should contain silica in a proportion of about 50 to 60 percent, alumina from 20 to 30 percent, and small quantities of lime, magnesia, iron oxide and alkalis. Silica prevents cracking and shrinkage and imparts hardness, while alumina imparts plasticity that makes the clay workable. Iron oxide acts as a flux and imparts the characteristic red colour to the brick, whereas lime in excess of the permitted limit causes the brick to melt and lose its shape during burning. Understanding the role of each constituent is essential because examination questions frequently ask which ingredient gives what property to a brick.

In this chapter we will study the constituents of good brick earth, the complete manufacturing process of clay bricks in stages, the classification of bricks into first, second and third class, the standard sizes prescribed by Indian Standard IS 1077, and the various field and laboratory tests such as compressive strength, water absorption, efflorescence and soundness. We will also discuss common defects in bricks and the examination points that recur most often, so that the candidate can revise the entire topic quickly and answer both theory and numerical questions with confidence.

2. Constituents of Good Brick Earth and Their Functions

The principal constituents of good brick earth are silica and alumina, and their relative proportions control the quality of the finished brick. Silica should be present in the range of 50 to 60 percent. It prevents shrinkage and cracking during drying and burning, imparts a uniform shape, and adds hardness to the brick. However, excess silica reduces cohesion between the particles and makes the brick brittle and weak. Alumina should be present in the range of 20 to 30 percent. It imparts plasticity, which is the property that allows wet clay to be moulded into shape, and it helps the clay to bind well. Excess alumina causes the raw brick to shrink, warp and crack on drying, and also makes the brick too sticky to handle.

Lime is desirable in small amounts not exceeding about 4 to 5 percent. A small quantity of lime acts as a flux that lowers the melting temperature and helps the silica to fuse, and it also imparts strength. But lime in excess causes the brick to melt and lose its shape in the kiln, and small particles of lime that remain unburnt swell when the brick absorbs moisture, causing the brick to blow or disintegrate. Iron oxide is present in the range of 5 to 6 percent and acts as a flux. It imparts the red colour and increases durability and impermeability, but excess iron oxide darkens the colour beyond an acceptable shade. Magnesia in small quantities imparts a yellow tint and reduces shrinkage, while alkalis are harmful because they cause efflorescence, the white crystalline deposit of salts that appears on the face of the brick after drying.

3. Manufacturing Process of Bricks

The manufacture of bricks involves four main stages: preparation of clay, moulding, drying and burning. In the first stage the clay is unsoaked, washed if required, and weathered in the open for a period of a few weeks to allow the impurities to be decomposed by air and rain. Tempering then follows, in which the clay is mixed with water and kneaded thoroughly, by hand or in a pug mill, to obtain a homogeneous plastic mass free from air voids. A good tempering operation produces clay of uniform consistency that can be moulded without cracking.

In the second stage the tempered clay is moulded into the shape of a brick either by hand or by machine. Hand moulding may be done on a table, called slop moulding, or on a ground, called ground moulding, and the mould is sprinkled with sand or water to prevent sticking. Machine moulding is of two types: plastic machine moulding, in which the plastic clay is extruded and cut to size, and dry press moulding, in which nearly dry clay is compacted under high pressure in steel moulds. Machine-made bricks are more regular in shape and stronger than hand-moulded bricks. The green bricks are then dried in the open, on a drying floor or in a hot-air dryer, to remove the moisture content to a safe limit before burning; drying prevents cracking and shrinkage during burning and is generally carried out for three to eight days.

The final and most important stage is burning, which may be done in a clamp or in a kiln. Burning removes all moisture, burns away the organic matter, and causes the silica to fuse sufficiently to bind the particles together and give the brick its hardness and strength. In a clamp, bricks are stacked in a pile with layers of fuel and burnt slowly, which takes a long time and gives bricks of uneven quality. Kilns are of two types: intermittent kilns such as the up-draught and down-draught kilns, and continuous kilns such as the Bull's trench kiln and the Hoffman kiln, which are used for large-scale production and give uniformly burnt bricks. The temperature of burning varies from about 800 degrees Celsius to 1200 degrees Celsius depending on the type of brick and the clay.

4. Classification, Standard Sizes and Tests of Bricks

Bricks are classified on the basis of quality into first class, second class, third class and over-burnt or Jhama bricks. First class bricks are well burnt, uniform in colour and shape, have a hard and ringing sound when struck, absorb water less than 20 percent of their dry weight, and have a minimum compressive strength of about 10.5 MPa as per IS 1077. Second class bricks are slightly over-burnt or under-burnt, have a somewhat irregular shape, absorb water up to about 22 percent, and are used where surface finish is not critical. Third class bricks are under-burnt and have a soft, earthy texture; they are used only for temporary and unimportant works. Over-burnt or Jhama bricks are vitrified, black in colour and irregular in shape, and are used in foundations where crushing strength is more important than appearance.

The standard brick sizes used in India must be remembered carefully. The conventional size of a brick is 190 mm x 90 mm x 90 mm, and with the addition of a 10 mm thick mortar joint the nominal modular size becomes 200 mm x 100 mm x 100 mm. In practice the commonly used traditional brick is 230 mm x 115 mm x 75 mm in size. The Indian Standard IS 1077 prescribes the modular size of 190 mm x 90 mm x 90 mm, and the weight of a standard brick is between 3.0 and 3.5 kg. The depression or indentation provided on the top face of a brick, called the frog, is 10 to 20 mm deep, and it holds the mortar during construction and also helps in keying successive courses of masonry.

The important tests on bricks include the compressive strength test, which is the crushing load divided by the area of the bed face, the water absorption test, in which the brick is immersed in water for 24 hours and the absorbed moisture must not exceed the prescribed limit of 20 percent for first class bricks, the efflorescence test for soluble salts, the hardness test by scratching with a knife, the soundness test by striking two bricks together, and the dimensional and shape tests. For a good brick, the edges should be sharp and square, the faces should be smooth and rectangular, the brick should not break when dropped from a height of about 1 metre, and the crushing strength of first class bricks should not be less than 10.5 MPa. When struck, a good brick should produce a clear metallic ringing sound.

5. Quick Revision Tables

Table 1: Constituents of Good Brick Earth and Their Functions

Constituent Percentage Function Effect of excess
Silica 50-60% Hardness, prevents cracking and shrinkage Brittleness, weak bond
Alumina 20-30% Plasticity, binding Shrinkage, warping, cracking
Lime 4-5% max Flux, strength Melting and loss of shape
Iron oxide 5-6% Red colour, durability Darkening of colour
Magnesia small Yellow tint, reduces shrinkage Reduction in strength

Table 2: Classification and Tests of Bricks

Class of brick Water absorption Minimum strength Typical use
First class less than 20% 10.5 MPa Exposed brickwork, permanent works
Second class up to 22% 7.5 MPa Internal walls, hidden work
Third class up to 25% 3.5 MPa Temporary works
Jhama (over-burnt) very low high crushing strength Foundations in wet locations
Test Acceptance criterion for good brick
Compressive strength Not less than 10.5 MPa for first class
Water absorption (24 h immersion) Not more than 20% of dry weight
Efflorescence No heavy whitish deposit on the face
Soundness Clear metallic ringing sound when struck
Hardness No scratch mark by a knife blade

6. Mind Map

flowchart TD
    A[Bricks] --> B[Good brick earth]
    A --> C[Manufacture]
    A --> D[Classification]
    A --> E[Tests]
    A --> F[Standard size]
    B --> B1[Silica 50-60% hardness]
    B --> B2[Alumina 20-30% plasticity]
    B --> B3[Lime small - flux]
    B --> B4[Iron oxide - colour]
    C --> C1[Preparation of clay]
    C --> C2[Moulding - hand or machine]
    C --> C3[Drying 3-8 days]
    C --> C4[Burning - clamp or kiln]
    D --> D1[First class]
    D --> D2[Second class]
    D --> D3[Third class]
    D --> D4[Jhama over-burnt]
    E --> E1[Compressive strength]
    E --> E2[Water absorption]
    E --> E3[Efflorescence]
    E --> E4[Soundness and hardness]
    F --> F1[190 x 90 x 90 mm IS 1077]
    F --> F2[Nominal 200 x 100 x 100 mm]

7. Important Diagrams (SVG)

The following diagrams summarise the stages of brick manufacture and the main parts of a standard brick.

Manufacturing Process of Clay Bricks 1. Unsoiling Remove top soil 2. Weathering Exposure to air 3. Tempering Kneading with water 4. Moulding Hand or machine 5. Drying 3 to 8 days 6. Burning Clamp or kiln 7. Cooling Slow cooling avoids cracks 8. Sorting and despatch First, second, third class and Jhama bricks Burning temperature ranges from 800 to 1200 degree Celsius. Golden Rule Always remember the order: clay preparation, moulding, drying and burning.

Standard Brick and Its Dimensions BED FACE 190 mm x 90 mm FROG (indentation 10-20 mm deep) Height 90 mm STRETCHER FACE 190 mm x 90 mm Length 190 mm IS 1077 modular size: 190 x 90 x 90 mm Nominal size with mortar: 200 x 100 x 100 mm Golden Rule A standard brick of 190 x 90 x 90 mm with a 10 mm joint gives the modular size 200 x 100 x 100 mm.

8. Common Mistakes

  1. Many students write the weight of a standard brick as 5 kg; the correct weight is between 3.0 and 3.5 kg, and this is frequently tested.
  2. A frequent error is to state the water absorption limit of first class bricks as 30 percent; the correct value is not more than 20 percent after 24 hours of immersion.
  3. Some candidates confuse the frog with a defect; the frog is an intentional depression on the top face that holds mortar and keys the courses together.
  4. Students often mix up the sizes and give the modular size as 230 mm x 115 mm x 75 mm; that is the traditional size, whereas IS 1077 prescribes 190 mm x 90 mm x 90 mm.
  5. It is wrong to say that alumina imparts hardness; hardness comes from silica, while alumina gives plasticity.
  6. A common mistake is to think that lime should be present in large quantity; excess lime causes the brick to melt and lose shape during burning.
  7. Many candidates believe that dry press moulding uses plastic clay; it uses nearly dry clay compacted under high pressure in steel moulds.
  8. Students frequently confuse the down-draught kiln with the Hoffman kiln as continuous types; the Hoffman and Bull's trench kilns are continuous, while the down-draught kiln is intermittent.

9. Exam Tips

  1. Memorise the IS 1077 modular brick size 190 x 90 x 90 mm and the nominal size 200 x 100 x 100 mm, since direct one-mark questions on size are extremely common.
  2. Remember the constituents in the order silica (50-60%), alumina (20-30%), lime and iron oxide, and attach one function to each constituent for quick recall.
  3. Learn the water absorption and compressive strength limits of first class bricks (20% and 10.5 MPa) because these numbers are asked repeatedly in both theory and numerical questions.
  4. Remember that the frog depth is 10 to 20 mm and that the frog is provided on the top face of the brick.
  5. Know the sequence of manufacturing stages (unsoiling, weathering, tempering, moulding, drying, burning, cooling) in the correct order.
  6. Remember that continuous kilns are the Bull's trench and Hoffman kilns, while the up-draught and down-draught kilns are intermittent types.
  7. Distinguish Jhama (over-burnt, black, used in foundations) from third class (under-burnt, soft, used for temporary works) bricks, because the two are often confused.
  8. In numerical questions on compressive strength, use the formula strength = crushing load divided by the bed face area, and convert units consistently.

10. Conclusion

Bricks form the most fundamental unit of masonry construction and are therefore an indispensable part of the Building Materials syllabus of every civil engineering examination. In this chapter we have studied the constituents of good brick earth and the role of each ingredient, the complete manufacturing process from clay preparation to burning, the classification of bricks into first, second, third and Jhama classes, the standard sizes prescribed by IS 1077, and the important field and laboratory tests including compressive strength, water absorption, efflorescence and soundness. We have also seen the common defects and the examination points that students most often get wrong. Because brick questions are short, factual and carry easy marks, a candidate who has memorised the sizes, percentages, limits and test criteria presented in this chapter can quickly secure full marks on this topic. The quick revision tables and the mind map given above summarise the entire chapter in a form that can be revised in a few minutes before the examination, making this material a valuable part of the preparation strategy.