Subject: Civil Engineering Chapter: Steel Structures Topic: 10.3 Welded Connections
Welding is the most widely used method of connecting steel members in modern construction because it produces a joint that is stronger, lighter and more rigid than a riveted joint. In a welded connection the adjoining edges of the members are fused together by intense local heat, with or without the addition of a filler material, so that the joint becomes essentially continuous and monolithic. Because no holes need to be punched and no bolts or rivets are used, the section is not weakened by holes, which means a welded joint can be made very efficient, often nearly as strong as the parent metal. Welded steel structures are used for bridges, buildings, transmission towers, industrial sheds, water tanks and pipe lines, and a large part of the steel structures syllabus of competitive examinations is devoted to welded connections.
The process of arc welding is the one most commonly used in structural steel work. In arc welding an electric arc is struck between the electrode and the work piece, and the intense heat of the arc, which can reach a temperature of about 3600 degree Celsius, melts the edges of the metal and the electrode together. The molten metal fuses and on cooling forms a strong joint. Depending on the relative positions of the two members, welded joints are classified as lap joints, butt joints, T-joints and corner joints, and the welds themselves are classified by the shape of their cross-section as fillet welds and butt or groove welds. The fillet weld, which has a triangular cross-section, is by far the most common weld in structural steel work because it can join members in any orientation.
In this chapter we will study the types of welded joints and welds, the symbols used to specify welds on drawings, the effective throat thickness and effective length of a fillet weld, the design strength of fillet and butt welds as per IS 800:2007, the stresses in welds, the defects that occur in welding, and the practical rules for welding such as minimum size and overlap. We will also solve worked examples on the design of a fillet weld required to carry a given tensile load. This chapter naturally follows the chapter on riveted and bolted connections, and it completes the study of the two main ways in which steel members are joined.
Welded joints are classified according to the relative position of the members being joined. A lap joint is formed when two plates overlap each other and are welded along the overlapping edges; a butt joint is formed when the two plates are placed edge to edge and welded along the gap between them; a T-joint is formed when one plate is placed perpendicular to another in the shape of the letter T; and a corner joint is formed when two plates meet at right angles like the corner of a box. Among these, lap and butt joints are the most important for design purposes.
The two principal types of welds are fillet welds and butt (groove) welds. A fillet weld has a triangular cross-section and is used to join two surfaces at right angles or at an angle, such as in a lap joint or a T-joint. The strength of a fillet weld is governed by its throat thickness, which is the minimum thickness of the triangular section, measured from the root of the weld to the hypotenuse joining the two legs. If the size of the weld leg is s, then the throat thickness is s divided by root2, that is, t = s/sin45 degrees = s/0.707 for a weld with equal legs. A butt weld is made by filling the gap between two plates placed edge to edge, and it is specified by the type of edge preparation, such as square butt, single V, double V, single U or double U, depending on the plate thickness.
The penetration of a weld is an important consideration. A full penetration butt weld, in which the weld metal extends through the full thickness of the plate, is designed as though the welded joint were the solid plate itself, using the plate thickness as the throat thickness. A fillet weld, however, is designed on the basis of its throat thickness, because the strength of the weld is proportional to the minimum section through which the load can be transmitted. The size of a fillet weld is defined as the length of the leg of the largest isosceles right triangle that can be inscribed in the weld cross-section. Fillet welds may be placed on one side of the plates, called a single fillet, or on both sides, called a double fillet.
As per IS 800:2007, the design strength of a fillet weld is based on the shear stress along the throat. The design shear strength per unit length of the weld is given by multiplying the throat thickness by the design shear strength of the weld metal, which is fu divided by (root3 x gamma_mw), where fu is the ultimate tensile stress of the parent metal and gamma_mw is the partial safety factor for welds, taken as 1.25. The throat thickness of a fillet weld is taken as 0.7 times the size of the weld, since 1/root2 is about 0.707. Thus, for a weld of size s, the throat thickness is 0.7s, and the design strength of the weld in shear per unit length is 0.7s x fu / (root3 x 1.25).
The effective length of a fillet weld is the length of the weld that actually contributes to carrying the load, and it is taken as the overall length minus twice the size of the weld, because the ends of the weld are less effective due to the crater and the tapering of the weld. The effective length of a fillet weld must not be less than four times the size of the weld. The strength of the weld is then the product of the design shear strength per unit length and the effective length. In a lap joint, if welds are provided on both sides, the two weld lengths are added together. The minimum size of a fillet weld depends on the thickness of the thickest plate, and the maximum size should not exceed the thickness of the thinner plate.
The design strength of a full penetration butt weld is taken as equal to the design strength of the parent metal, because the weld is assumed to be as strong as the plate. For a partial penetration butt weld, the throat thickness is the depth of penetration and the weld is designed like a fillet weld, with the strength based on the throat. In the design of connections, it is normally assumed that the load is transferred evenly along the length of the weld, but in practice the stresses are higher at the ends, which is why the effective length is reduced. The connection is designed so that the total strength of all the welds is at least equal to the load to be transmitted.
A lap joint is required to transmit a load of 150 kN through a fillet weld on both sides. The size of the weld is 8 mm and the ultimate stress of steel is 410 N/mm2. Determine the effective length of weld required on each side. Take gamma_mw = 1.25.
Solution: Throat thickness, t = 0.7 x s = 0.7 x 8 = 5.6 mm. Design shear strength of weld = fu / (root3 x gamma_mw) = 410 / (1.732 x 1.25) = 189.37 N/mm2. Strength of weld per unit length = 5.6 x 189.37 = 1060.5 N/mm. Total effective length required = Load / strength per unit length = 150000 / 1060.5 = 141.4 mm. Since welds are on both sides, effective length on each side = 141.4 / 2 = 70.7 mm. Add twice the size of the weld for overall length: overall length = 70.7 + 16 = 86.7 mm on each side.
In a welded connection the stresses developed are shear stress along the throat of a fillet weld and tensile, compressive or shear stress across a butt weld. For a fillet weld under eccentric load, the weld is subjected to a combination of direct shear and torsional shear due to the eccentricity, and the resultant stress must be found by vector addition and kept within the permissible value. For a bracket connection welded to the flange of a column, the weld must resist both the vertical load and the moment caused by the eccentricity of the load. The maximum resultant stress in the weld is the vector sum of the direct shear stress and the shear stress due to the twisting moment, and this resultant must not exceed the design shear strength of the weld.
Welding defects reduce the strength of a joint and must be avoided by proper procedure and inspection. The common defects are incomplete penetration, in which the weld metal does not fuse with the root of the joint; porosity, caused by gas bubbles trapped in the weld metal; slag inclusion, in which slag is trapped inside the weld; undercut, which is a groove melted into the base metal along the toe of the weld; and cracks, which may occur during cooling or later under service load. Welding distortion and residual stresses are also produced because the weld metal shrinks on cooling, and they are reduced by proper edge preparation, preheating, welding sequence and the use of symmetrical welds.
There are several practical rules for welding that a candidate must remember. The minimum size of a fillet weld should not be less than 3 mm. The effective length of a fillet weld must not be less than four times its size. The maximum size of a fillet weld is limited by the thickness of the thinner plate, and the minimum size depends on the thickness of the thicker plate. The overlapping of plates in a lap joint should be at least five times the thickness of the thinner plate to keep the eccentricity small, but not more than the necessary value. Welds should be placed symmetrically with respect to the centroidal axis of the connected members wherever possible, so that the joint does not become eccentric. The design of a weld is always governed by the smaller of the weld strength and the plate strength.
| Type of Weld | Cross-section | Design Basis | Typical Use |
|---|---|---|---|
| Fillet weld | Triangular | Throat thickness 0.7s | Lap and T-joints |
| Full penetration butt weld | Groove filled | Plate thickness | Edge to edge joints |
| Partial penetration butt weld | Partial groove | Penetration depth | Heavy plates |
| Plug / slot weld | Filled hole | Shear of weld | Lap joints, stiffeners |
| Quantity | Expression | Value for s = 8 mm |
|---|---|---|
| Throat thickness | t = 0.7 x s | 5.6 mm |
| Shear strength per unit area | fu / (root3 x 1.25) | 189.37 N/mm2 |
| Strength per unit length | t x 189.37 | 1060.5 N/mm |
| Minimum effective length | 4 x s | 32 mm |
| Effective length | Overall length - 2s | L - 16 mm |
flowchart TD
A[Welded Connections] --> B[Types of joints]
A --> C[Types of welds]
A --> D[Design of fillet weld]
A --> E[Design of butt weld]
A --> F[Defects and rules]
B --> B1[Lap, butt, T and corner joints]
C --> C1[Fillet weld - throat 0.7s]
C --> C2[Butt weld - plate thickness]
D --> D1[Design shear strength fu/(root3 x 1.25)]
D --> D2[Effective length = L - 2s]
E --> E1[Full penetration = parent metal]
E --> E2[Partial penetration = like fillet]
F --> F1[Porosity, slag, cracks, undercut]
F --> F2[Minimum size 3 mm, effective length >= 4s]
The following diagrams show the cross-section of a fillet weld with its throat thickness, and the typical welded joints used in steel structures.
Welded connections have replaced riveted connections as the primary method of joining steel members because they give stronger, lighter and more rigid joints. In this chapter we have studied the different types of welded joints, namely lap, butt, T and corner joints, and the two main types of welds, the fillet weld and the butt weld. We have seen that the strength of a fillet weld depends on its throat thickness, which is 0.7 times the weld size, and on the design shear strength of the weld metal, which is fu/(root3 x 1.25). We have solved a worked example on finding the required length of a fillet weld for a given load, and we have examined the effective length rules, the minimum and maximum weld sizes, the common welding defects and the practical rules for good welding practice. The design philosophy of checking the weld against the load with proper safety factors is the same as that used for riveted and bolted connections, and the same logic of effective area and permissible stress runs through the entire steel structures syllabus. A candidate who is comfortable with throat thickness calculations and the effective length rules will find the numerical questions of this chapter quick and easy to solve.