🏗️ Civil Engineering

22.6 Pavement Materials

Start MCQ Practice →

22.6 Pavement Materials

Subject: Civil Engineering Chapter: Transportation Engineering Topic: 22.6 Pavement Materials

1. Introduction

A pavement is a layered structure that spreads the wheel loads of the traffic over the subgrade soil, and the quality of the materials used in its layers decides the performance, the life and the maintenance cost of the road. The materials used in highway construction are the subgrade soil, the aggregates used in the base and surface courses, the bitumen used as a binder in flexible pavements, and the cement used in rigid pavements. Since the pavement must resist heavy wheel loads, abrasion, weathering and the action of water, every material must satisfy the standard tests and specifications laid down by the Indian Roads Congress and the Bureau of Indian Standards.

The choice of material and the strict control of its quality are the most important steps in ensuring a durable pavement. Poor aggregates crumble under traffic, weak soil settles under the pavement, and inferior bitumen becomes brittle in winter and soft in summer, so a candidate must know the tests that detect each of these defects and the limiting values specified for each test. Questions on the standard values of the Los Angeles abrasion value, the aggregate impact value, the penetration grade of bitumen and the California Bearing Ratio appear repeatedly in examinations.

In this chapter we will study the properties and tests of the subgrade soil, the aggregates and the bituminous binders, with the standard test procedures and the specified limits, and we will solve numerical problems on the computation of the abrasion value, the impact value and the CBR. The chapter thus provides the material knowledge that is applied directly in the design of flexible and rigid pavements in the following chapters.

2. Subgrade Soil and Its Tests

The subgrade is the natural soil prepared to receive the pavement, and it must provide a stable foundation for the pavement layers above it. The important soil properties studied in highway engineering are the grain size distribution, the Atterberg limits, the compaction characteristics, the bearing capacity and the California Bearing Ratio. The grain size distribution shows the proportions of gravel, sand, silt and clay, and it is obtained by the sieve analysis and the hydrometer analysis. The Atterberg limits, namely the liquid limit, the plastic limit and the shrinkage limit, describe the consistency of the fine-grained soil and its behaviour with water, and the plasticity index is the difference between the liquid limit and the plastic limit.

The compaction of the subgrade is carried out at the optimum moisture content to obtain the maximum dry density, and the relationship between the moisture content and the dry density is obtained from the standard Proctor test and the modified Proctor test. Compaction increases the density and the strength of the soil and reduces its settlement and permeability, so the subgrade is compacted to the specified density within the permissible moisture content range. The California Bearing Ratio test measures the bearing capacity of the subgrade for pavement design; a sample is compacted in the laboratory, soaked for four days to simulate the worst field condition, and then penetrated by a standard plunger.

The CBR value is expressed as the ratio of the test load to the standard load, multiplied by 100, and it is computed at both the 2.5 mm and 5 mm penetrations, taking the higher of the two values. The standard loads are 13.7 kN at 2.5 mm penetration and 20.5 kN at 5 mm penetration. The soaked CBR of the subgrade is used directly in the design charts of the pavement thickness, so a high CBR soil gives a thinner and cheaper pavement. For a typical subgrade the CBR may range from 2 percent for very poor clay to 20 percent or more for good sandy soil.

Solved Problem 1: In a CBR test, the load on the plunger at 2.5 mm penetration is 10.275 kN and at 5 mm penetration is 16.4 kN. Determine the CBR value. Solution: CBR at 2.5 mm = 10.275/13.7 x 100 = 75 percent. CBR at 5 mm = 16.4/20.5 x 100 = 80 percent. The CBR is taken as the higher value, which is 80 percent.

3. Aggregates and Their Tests

Aggregates form about 90 percent of the volume of a bituminous pavement and about 75 percent of the volume of a cement concrete pavement, so their quality has a decisive influence on the pavement. The aggregates used in the base course and the surface course must have adequate strength to resist the crushing under the wheel loads, sufficient hardness to resist abrasion by the traffic, enough toughness to resist the impact of falling loads, and a good shape so that the stones interlock properly. The important tests on aggregates are the crushing strength test, the Los Angeles abrasion test, the aggregate impact test, the shape tests giving the flakiness and elongation indices, and the tests for specific gravity and water absorption.

The Los Angeles abrasion test measures the resistance of the aggregate to abrasion and impact; a sample of the specified size is placed in the Los Angeles machine with steel balls and rotated for 500 revolutions, and the percentage of the material worn away is computed. The Los Angeles abrasion value should not exceed 30 percent for the surface course of a bituminous road and about 40 to 50 percent for the base course. The aggregate impact test measures the resistance to sudden impact; the sample is subjected to 15 blows of a hammer in the impact machine, and the fines passing the 2.36 mm sieve are expressed as a percentage of the sample, giving the aggregate impact value which should not exceed 30 percent for the surface course.

The shape of the aggregate is described by the flakiness index and the elongation index. A flaky aggregate is one whose thickness is less than 0.6 times its mean dimension, and an elongated aggregate is one whose length is more than 1.8 times its mean dimension; both shapes break easily and reduce the interlock, so the flakiness index and the elongation index should not exceed 15 percent for the surface course. The aggregate should also be free from dust, clay and organic matter, and its water absorption should be low, since the absorbed water weakens the bond with the bitumen.

Solved Problem 2: In a Los Angeles abrasion test, 5000 g of aggregate is placed in the machine and after 500 revolutions the material retained on the 1.7 mm sieve is 4100 g. Find the abrasion value. Solution: Loss = 5000 - 4100 = 900 g. Los Angeles abrasion value = (900/5000) x 100 = 18 percent.

Solved Problem 3: In an aggregate impact test, 350 g of aggregate passing the 12.5 mm sieve and retained on the 10 mm sieve is subjected to impact, and 70 g of the fines passes the 2.36 mm sieve. Find the aggregate impact value. Solution: AIV = (70/350) x 100 = 20 percent.

4. Bitumen and Bituminous Binders

Bitumen is a dark, thermoplastic material obtained from the distillation of petroleum, and it acts as the binder in flexible pavements, holding the aggregates together and providing a waterproofing film. The quality of bitumen is specified by its consistency, purity, safety and temperature susceptibility, and the standard tests are the penetration test, the softening point test, the ductility test, the flash and fire point tests, the viscosity test and the specific gravity test. The penetration test measures the hardness of the bitumen: a standard needle of 100 g weight is allowed to penetrate the sample at 25 degrees Celsius for 5 seconds, and the penetration is expressed in units of one-tenth of a millimetre.

The penetration grades of bitumen used in India are 30/40, 60/70 and 80/100, in which the numbers give the range of the penetration value; a higher penetration number means a softer bitumen. The viscosity of the bitumen is measured by the kinematic viscosity test at 60 degrees Celsius, and the current specifications use the viscosity grades VG10, VG20, VG30 and VG40, of which VG30 is the most commonly used for normal roads. The softening point test, using the ring and ball apparatus, gives the temperature at which the bitumen softens and becomes fluid; for paving bitumen it is about 45 to 50 degrees Celsius, and a higher softening point indicates a lower temperature susceptibility.

The ductility test measures the distance in centimetres to which the bitumen can be stretched at 27 degrees Celsius before it breaks; the ductility of paving bitumen should be at least 50 cm. The flash point is the lowest temperature at which the vapours of the heated bitumen momentarily catch fire, and the fire point is the temperature at which the bitumen itself catches fire; the flash point of bitumen should be above 175 degrees Celsius for safety during heating. The specific gravity of bitumen is about 1.01, and bitumen is virtually impervious to water. Bitumen emulsions, which are the suspension of bitumen globules in water, and cutback bitumen, which is bitumen dissolved in a solvent, are also used in construction and surface dressing.

5. Quick Revision Tables

Table 1: Tests on Subgrade Soil and Aggregates

Material Test Purpose Typical limit
Soil CBR test Bearing capacity Used in design charts
Soil Standard Proctor test Optimum moisture content and density Field compaction control
Aggregate Los Angeles abrasion Resistance to abrasion Max 30 percent surface course
Aggregate Aggregate impact Resistance to impact Max 30 percent surface course
Aggregate Flakiness index Shape control Max 15 percent surface course
Aggregate Specific gravity Quality and voids About 2.6

Table 2: Tests on Bitumen

Test Apparatus Value for paving bitumen
Penetration test Penetrometer 30/40, 60/70, 80/100 grades
Softening point Ring and ball About 45 to 50 degrees C
Ductility test Ductility machine Minimum 50 cm at 27 degrees C
Flash point Pensky-Martens / Cleveland Above 175 degrees C
Viscosity Viscometer at 60 degrees C VG30 common grade
Specific gravity Pycnometer About 1.01

6. Mind Map

flowchart TD
    A[Pavement Materials] --> B[Subgrade soil]
    A --> C[Aggregates]
    A --> D[Bitumen]
    A --> E[Cement and water]
    B --> B1[Compaction OMC and MDD]
    B --> B2[Atterberg limits]
    B --> B3[CBR test]
    C --> C1[Los Angeles abrasion]
    C --> C2[Aggregate impact]
    C --> C3[Flakiness and elongation]
    D --> D1[Penetration grades]
    D --> D2[Softening point]
    D --> D3[Ductility]
    D --> D4[Flash point]
    B3 --> F[CBR at 2.5 and 5 mm penetration]
    C1 --> G[Max 30 percent for surface course]
    D1 --> H[30/40, 60/70, 80/100]
    F --> I[Higher CBR gives thinner pavement]

7. Important Diagrams (SVG)

The following diagrams show the load-penetration curve of the CBR test and the arrangement of the ring and ball apparatus used for the softening point test of bitumen.

Load-Penetration Curve of the CBR Test Penetration (mm) Load (kN) 2.5 mm Test load CBR = (Test load / Standard load) x 100 Standard loads: 13.7 kN at 2.5 mm, 20.5 kN at 5 mm Golden Rule CBR is the higher of the values at 2.5 mm and 5 mm penetration, using standard loads.

Ring and Ball Apparatus (Softening Point Test) SUPPORT PLATE Ring Ring Steel balls WATER BATH Temperature rises at 5 degrees C per minute Softening point is the temperature at which the ball touches the bottom plate together with the bitumen For paving bitumen about 45 to 50 degrees C Golden Rule Softening point indicates temperature susceptibility of bitumen, measured by the ring and ball test.

8. Common Mistakes

  1. Many students use the load at 5 mm alone as the CBR, forgetting that the higher of the 2.5 mm and 5 mm values is adopted.
  2. A frequent error is to use the standard load of 13.7 kN at 5 mm penetration; the 13.7 kN standard load corresponds to 2.5 mm penetration.
  3. Some candidates state that the penetration value of bitumen is measured in millimetres; it is measured in units of one-tenth of a millimetre.
  4. Students often confuse the penetration grade with the viscosity grade; the penetration grades are 30/40, 60/70 and 80/100, while the viscosity grades are VG10 to VG40.
  5. A common mistake is to state the ductility limit of bitumen as 25 cm; it is a minimum of 50 cm at 27 degrees Celsius.
  6. Many candidates forget that the Los Angeles abrasion value for the surface course should not exceed 30 percent and quote 50 percent.
  7. Some students compute the aggregate impact value by dividing the retained material by the sample weight instead of the fines passing the 2.36 mm sieve.
  8. Another recurring error is to test the subgrade CBR in the dry condition; the sample is soaked for four days before penetration.

9. Exam Tips

  1. Memorise the CBR standard loads: 13.7 kN at 2.5 mm and 20.5 kN at 5 mm penetration.
  2. Remember that the maximum Los Angeles abrasion value is 30 percent for the surface course and 40 to 50 percent for the base.
  3. Learn the bitumen penetration grades 30/40, 60/70 and 80/100, and the viscosity grades VG10 to VG40.
  4. Note the ductility limit of 50 cm at 27 degrees Celsius and the flash point above 175 degrees Celsius.
  5. For the aggregate impact value, the permissible maximum is 30 percent for the surface course.
  6. Remember the flakiness and elongation index limits of 15 percent for the surface course.
  7. In compaction, associate the maximum dry density with the optimum moisture content obtained from the Proctor test.
  8. Always express the Los Angeles abrasion value as a percentage loss and the CBR as a percentage ratio of the standard load.

10. Conclusion

The materials of a pavement decide its cost, its life and its performance under traffic, so the testing and control of soil, aggregates and bitumen form an essential part of highway engineering. In this chapter we have studied the subgrade soil and its tests, including the compaction test and the California Bearing Ratio test, the aggregates and their tests, including the Los Angeles abrasion, aggregate impact and shape tests, and the bituminous binders with their penetration, softening point, ductility and flash point tests. The standard values and the limiting specifications of each material have been presented in a form that can be memorised easily, and the worked examples have demonstrated the computation of the CBR, the Los Angeles abrasion value and the aggregate impact value. This material knowledge now equips the candidate to understand the structural design of pavements, because the thickness and composition of the flexible and rigid pavements described in the next two chapters depend directly on the values of these material tests.

(End of file - total 165 lines)