Subject: ICSE Class 10 Chemistry Chapter: Aluminium Extraction Topic: 7.6 Aluminium Extraction – Study purification of bauxite by Baeyer process
Aluminium is the most abundant metal in the earth's crust, yet for a very long time it was considered a precious metal because it was extremely difficult to extract. The reason is that aluminium is a highly reactive metal, placed high in the reactivity series, and it has a very strong affinity for oxygen. It cannot be extracted by reducing its oxide with carbon, hydrogen, or carbon monoxide. Aluminium can only be obtained from its oxide by the process of electrolysis, which uses a large amount of electrical energy.
The ore of aluminium is bauxite, which has the formula Al2O3.2H2O. However, bauxite as mined is never pure. It contains impurities such as iron oxide (Fe2O3) and silica (SiO2). If these impurities are not removed, the aluminium extracted will be impure, and the impurities would also interfere with the electrolytic process. Therefore, the bauxite must first be purified, and the method used for this purification is called the Baeyer process.
In this chapter we will study the purification of bauxite by the Baeyer process. We will learn why bauxite is purified, how aluminium hydroxide is precipitated and converted to pure alumina, and how the alumina is then used in the electrolytic extraction of aluminium. The Baeyer process uses sodium hydroxide solution to separate aluminium oxide from the impurities of iron oxide and silica.
The Baeyer process is the method used to purify bauxite to obtain pure aluminium oxide or alumina. The impure bauxite is first crushed and powdered, and then it is treated with a concentrated solution of sodium hydroxide. Since aluminium oxide is amphoteric in nature, it dissolves in sodium hydroxide to form sodium aluminate, while the impurities of iron oxide and silica do not behave in the same way and are removed.
The steps of the Baeyer process are as follows. The powdered bauxite is digested with a hot concentrated solution of sodium hydroxide under pressure. The aluminium oxide dissolves to form sodium aluminate, which is soluble in water. The iron oxide impurity, being basic and insoluble in sodium hydroxide, remains undissolved and is filtered off. The silica impurity dissolves in the sodium hydroxide to form sodium silicate, and it is also removed in a later step.
Step 1: The powdered bauxite is mixed with a hot concentrated solution of sodium hydroxide and heated under pressure in a digester. The aluminium oxide present in bauxite dissolves to form sodium aluminate. The reaction is Al2O3 + 2NaOH gives 2NaAlO2 + H2O.
Step 2: The insoluble impurities such as iron oxide settle down and are removed by filtration. The sodium aluminate solution, which is clear, is then diluted with water. When the solution is diluted and seeded, aluminium hydroxide precipitates out, while the sodium silicate remains in solution.
Step 3: The precipitated aluminium hydroxide is filtered, washed, and then heated strongly to remove water. On heating, aluminium hydroxide decomposes to give pure aluminium oxide or alumina. The reaction is 2Al(OH)3 gives Al2O3 + 3H2O. This pure alumina is then used for the electrolytic extraction of aluminium.
The principle of the Baeyer process is the amphoteric nature of aluminium oxide. Aluminium oxide can behave both as an acid and as a base, so it dissolves in sodium hydroxide. Iron oxide is only basic and does not dissolve in sodium hydroxide, so it is removed by filtration. Silica forms sodium silicate which remains in solution and is separated from the aluminium hydroxide precipitate.
The Baeyer process depends on the following key reactions, and the conditions are carefully controlled for each one. The digestion is carried out at a high temperature and under pressure because the reaction of aluminium oxide with sodium hydroxide is favoured by these conditions. Dilution with water is used to bring about the precipitation of aluminium hydroxide, and seeding helps the precipitation to be faster and more complete.
Reaction with sodium hydroxide: Al2O3 + 2NaOH gives 2NaAlO2 + H2O. In this reaction the amphoteric aluminium oxide dissolves in sodium hydroxide forming soluble sodium aluminate, while the basic impurity iron oxide does not dissolve.
Precipitation of aluminium hydroxide: When the sodium aluminate solution is diluted with water and a little of the fresh aluminium hydroxide is added as seed, the aluminium hydroxide precipitates. The reaction is NaAlO2 + 2H2O gives Al(OH)3 + NaOH. The sodium hydroxide formed is recovered and reused, which makes the process economical.
Decomposition by heating: The aluminium hydroxide is heated strongly to about 1000 degrees Celsius, and it decomposes to give pure alumina. The reaction is 2Al(OH)3 gives Al2O3 + 3H2O. The alumina obtained is a white powder that is insoluble in water and is now ready for electrolysis.
The recovered sodium hydroxide is recycled in the process, which reduces the cost. The whole purpose of the Baeyer process is to get pure alumina free from iron oxide and silica. Pure alumina is essential because in the electrolytic extraction, iron and silicon would contaminate the aluminium if the alumina were not pure. The purity of the alumina also determines the purity of the aluminium obtained.
The pure alumina obtained from the Baeyer process is the starting material for the extraction of aluminium. Alumina is a white powder with a very high melting point of about 2050 degrees Celsius. Because of this very high melting point, alumina alone cannot be melted easily for electrolysis, and this is why another substance called cryolite is used to lower the melting point in the Hall Heroult process.
The purification of bauxite is essential for several reasons. First, the impurities of iron oxide and silica would contaminate the aluminium metal if they remained in the ore. Second, the impurities would consume a part of the electric current and reduce the efficiency of the electrolytic cell. Third, the presence of iron oxide in the anode would cause the burning of the carbon anodes. Therefore, the bauxite is always purified before electrolysis.
Key points about purified alumina: - It is a white powder, insoluble in water. - Its formula is Al2O3, and it is called alumina. - It has a very high melting point of about 2050 degrees Celsius. - It is dissolved in molten cryolite to lower the melting point before electrolysis. - Pure alumina is essential to get pure aluminium.
The Baeyer process is the most commonly used method for the purification of bauxite in the ICSE syllabus. Students should remember the three main steps: dissolution in sodium hydroxide, precipitation of aluminium hydroxide on dilution, and conversion of the hydroxide to pure alumina by strong heating. These three steps together give the pure alumina that is used in the next chapter's Hall Heroult process.
The steps of the Baeyer process:
| Step | Treatment | Product Obtained |
|---|---|---|
| Digestion | Bauxite with hot NaOH under pressure | Sodium aluminate solution |
| Filtration | Removes insoluble iron oxide | Clear sodium aluminate solution |
| Dilution and seeding | Water and fresh hydroxide seed | Aluminium hydroxide precipitate |
| Strong heating | Aluminium hydroxide at about 1000 C | Pure alumina Al2O3 |
Impurities of bauxite and their removal:
| Impurity | Behaviour with NaOH | How Removed |
|---|---|---|
| Aluminium oxide Al2O3 | Dissolves to form sodium aluminate | Goes into solution |
| Iron oxide Fe2O3 | Does not dissolve | Removed by filtration |
| Silica SiO2 | Forms sodium silicate | Remains in solution on dilution |
| Aluminium hydroxide | Precipitates on dilution | Collected as precipitate |
flowchart TD
A[Aluminium Extraction] --> B[Bauxite Al2O3.2H2O]
B --> C[Baeyer process purification]
C --> D[Bauxite with hot NaOH]
D --> E[Sodium aluminate]
E --> F[Iron oxide filtered off]
E --> G[Dilution and seeding]
G --> H[Aluminium hydroxide precipitate]
H --> I[Strong heating]
I --> J[Pure alumina Al2O3]
J --> K[Electrolysis Hall Heroult]
The first diagram shows the flow of the Baeyer process for purifying bauxite, and the second diagram shows the amphoteric behaviour of aluminium oxide that makes the process possible.
Aluminium, being a highly reactive metal, cannot be reduced by carbon and must be obtained by electrolysis of its oxide. Before this electrolysis can be carried out, the bauxite ore must be purified by the Baeyer process, in which the amphoteric aluminium oxide is dissolved in hot sodium hydroxide to form sodium aluminate, the iron oxide impurity is removed by filtration, and the aluminium hydroxide precipitated on dilution is converted to pure alumina by strong heating. The pure alumina so obtained is the starting material for the electrolytic extraction of aluminium. We are now ready to study the Hall Heroult process, in which this purified alumina is dissolved in molten cryolite and electrolysed to obtain aluminium metal.