Subject: Inorganic Chemistry Chapter: Metallurgy Topic: 14.2 Ore Concentration – Study physical methods of ore enrichment
The ore obtained from the mines contains a large amount of unwanted earthy and rocky material called gangue. Before the metal can be extracted from the ore, this gangue must be removed so that the percentage of the metal compound in the ore increases. This preliminary step of removing gangue from the ore is called concentration, dressing or beneficiation of the ore. Concentration is always the first operation in metallurgy because it is carried out by physical methods that are cheap and simple, and because removing the gangue early prevents the wasteful consumption of fuel, reducing agents and reagents in the later chemical stages of extraction.
The choice of the concentration method depends entirely on the difference between some physical property of the ore particles and that of the gangue particles. If the ore is heavier than the gangue, gravity separation is used; if one of the components is magnetic, magnetic separation is used; and if the ore particles are wetted by oil but not by water, froth floatation is used. In every method the basic principle is the same: create a condition in which the ore particles and the gangue particles behave differently, and then use that difference to separate them. For a competitive examination candidate, this topic is a rich source of one-mark questions that test the principle and the application of each method.
In this chapter we will study the main physical methods of ore concentration, namely hydraulic washing, gravity separation or levigation, magnetic separation and froth floatation. We will also examine the process of leaching, which is a chemical method of concentration used for certain ores such as bauxite. By the end of this chapter the student should be able to match every important ore with the correct concentration method and explain the physical principle on which each method is based.
Hydraulic washing is a method of ore concentration based on the difference in the densities of the ore particles and the gangue particles. In this method, a stream of water is allowed to flow over the powdered ore placed on a sloping surface. The lighter gangue particles are carried away by the flowing water, while the heavier ore particles remain behind. This method is also called levigation, and it is used for ores whose metallic compound is heavier than the gangue. Oxide ores such as haematite, cassiterite and gold-bearing ores are generally concentrated by this method.
In the hydraulic classifier, the powdered ore is fed into the top of a device in which a stream of water rises from the bottom. The heavier ore particles settle at the bottom because they cannot be lifted by the water current, while the lighter gangue particles are carried upward and out with the overflowing water. The velocity of the rising water can be adjusted so that the separation becomes efficient. Hydraulic washing is one of the oldest methods of concentration and was used in gold panning, where the heavy gold particles remain in the pan while lighter sand is washed away.
Gravity separation is a more general name for methods in which the heavier ore particles are separated from the lighter gangue by the action of gravity, sometimes assisted by a moving medium such as water or air. The specific gravity of the ore and gangue must differ significantly for the method to work. For example, the gangue in tin ore is lighter than cassiterite, so a stream of water easily separates them. This method is simple, cheap and does not require any chemicals, which is why it is always tried first before the more expensive methods are considered.
Magnetic separation is a method of concentration based on the difference in the magnetic properties of the ore particles and the gangue particles. In this method, the finely ground ore is made to fall on a moving belt that passes around two rollers, one of which is a powerful electromagnet. The magnetic particles in the ore stick to the belt near the magnetic roller and are carried a little further, where they drop into a separate container, while the non-magnetic gangue particles fall off the belt nearer the point of feeding. In this way the magnetic ore is separated from the non-magnetic gangue.
Magnetic separation is used when either the ore or the gangue is magnetic. It is used in the concentration of ores such as magnetite, Fe3O4, which is magnetic, and for removing magnetic impurities of iron like tinstone from non-magnetic tin ore. The method is particularly valuable in the concentration of low-grade ores, where the difference in magnetic susceptibility between the ore and the gangue allows a clean separation even when the density difference is small.
The efficiency of magnetic separation depends on the degree of magnetism of the particles and on the strength of the magnetic field. Weakly magnetic minerals can also be separated by using very strong electromagnets. In the separation of tinstone (cassiterite) from the wolframite impurity, the wolframite is magnetic and is attracted, leaving pure cassiterite. Magnetic separation is thus one of the cleanest physical methods, as it can remove even traces of iron impurities from ores and from the products of industrial processes.
Froth floatation is the most important and most widely used method for concentrating sulphide ores, because it exploits the difference in the wetting properties of the ore particles and the gangue particles by water. In this method, the finely ground ore is mixed with water in a large tank, and a small quantity of a frothing agent such as pine oil is added. Air is then blown through the mixture with a strong current, producing a large amount of froth or foam on the surface of the water. The sulphide ore particles, being preferentially wetted by the oil, attach themselves to the air bubbles and rise with the froth to the surface, while the gangue particles, being wetted by water, settle at the bottom.
The particles of the ore that collect in the froth are skimmed off and the froth is broken down by washing with water to get the concentrated ore. To make the separation more efficient, a substance called a collector is added, which selectively makes the ore particles water-repellent or hydrophobic. Collectors such as ethyl xanthate are commonly used. In addition, a small quantity of a depressant may be added to prevent certain minerals from coming to the froth, a technique used in the separation of lead and zinc sulphides, where sodium cyanide depresses the zinc blende while the galena floats.
Froth floatation is used for the concentration of sulphide ores such as copper pyrites, zinc blende, galena and cinnabar. The method is based on the fact that sulphide ores are preferentially wetted by oil while the gangue is wetted by water. This selective wetting is the key principle, and it is this principle, not density or magnetism, that makes froth floatation the standard method for sulphide ores. The froth floatation process can also be used to separate two sulphide ores from each other by the use of suitable depressants, as in the case of galena and zinc blende.
Leaching is a chemical method of concentration in which the powdered ore is treated with a suitable reagent that dissolves the metallic compound but not the gangue. The solution containing the dissolved metal compound is then filtered to remove the undissolved gangue, and the metal compound is recovered from the solution. Leaching is used when physical methods of concentration fail, especially for ores in which the metal compound is soluble in a particular reagent.
The most important example of leaching is the concentration of bauxite ore by the Bayer process. In this process, the powdered bauxite is treated with a hot concentrated solution of sodium hydroxide, which dissolves the aluminium oxide as sodium aluminate, leaving behind the insoluble impurities of iron oxide and silica. The solution is then filtered, and aluminium hydroxide is precipitated from the filtrate by passing carbon dioxide through it, after which it is filtered, washed and ignited to obtain pure alumina.
Leaching is also used for the recovery of gold and silver from their low-grade ores. In the cyanide process, the crushed gold ore is treated with a dilute solution of sodium cyanide in the presence of air, which dissolves the gold forming a soluble complex. The gold is then precipitated from the solution by adding zinc dust. Leaching is thus a versatile concentration method, and although it is called a chemical method, it serves the same purpose as the physical methods, namely the separation of the metal compound from the gangue before the main reduction step.
| Method | Principle | Ores concentrated | Key reagent |
|---|---|---|---|
| Hydraulic washing / levigation | Difference in densities | Haematite, cassiterite, gold ore | Flowing water |
| Gravity separation | Difference in specific gravity | Heavy oxide ores | Water or air current |
| Magnetic separation | Difference in magnetic properties | Magnetite, tinstone from wolframite | Electromagnet |
| Froth floatation | Difference in wetting by water and oil | Copper pyrites, zinc blende, galena | Pine oil, ethyl xanthate |
| Leaching | Chemical dissolution of ore | Bauxite, gold, silver ores | NaOH, NaCN solution |
| Ore | Concentration method | Why the method works |
|---|---|---|
| Haematite Fe2O3 | Hydraulic washing | Ore heavier than gangue |
| Cassiterite SnO2 | Gravity separation / magnetic separation | Gangue lighter; wolframite is magnetic |
| Magnetite Fe3O4 | Magnetic separation | Ore itself is magnetic |
| Copper pyrites CuFeS2 | Froth floatation | Sulphide wetted by oil, gangue by water |
| Zinc blende ZnS | Froth floatation | Sulphide ore particles become hydrophobic |
| Galena PbS | Froth floatation | Floats in froth; zinc blende depressed by NaCN |
| Bauxite Al2O3.2H2O | Leaching (Bayer process) | Alumina dissolves in NaOH, impurities do not |
| Gold ore | Leaching (cyanide process) | Gold dissolves in NaCN solution in presence of air |
flowchart TD
A[Ore Concentration] --> B[Hydraulic washing]
A --> C[Gravity separation]
A --> D[Magnetic separation]
A --> E[Froth floatation]
A --> F[Leaching]
B --> B1[Based on density difference]
B --> B2[Used for haematite, gold ore]
B --> B3[Also called levigation]
C --> C1[Heavier ore settles, gangue washed away]
C --> C2[Used for cassiterite]
D --> D1[Electromagnet roller]
D --> D2[Used for magnetite]
D --> D3[Removes wolframite from tinstone]
E --> E1[Sulphide ores wetted by oil]
E --> E2[Pine oil creates froth]
E --> E3[Collector ethyl xanthate]
E --> E4[Depressant NaCN separates PbS and ZnS]
F --> F1[Chemical method]
F --> F2[Bayer process for bauxite]
F --> F3[Cyanide process for gold]
A --> G[Principle: difference in physical properties]
The following diagrams show the working principles of the froth floatation and magnetic separation methods used for the concentration of ores.
The concentration of an ore is the essential preliminary step of metallurgy in which the worthless gangue is removed so that the subsequent chemical operations act only on the valuable metal compound. In this chapter we have studied the physical methods of hydraulic washing and gravity separation, which use differences in density, magnetic separation, which uses differences in magnetic properties, and froth floatation, which uses the selective wetting of sulphide ore particles by oil. We have also examined leaching, the chemical method used for ores such as bauxite and gold-bearing rocks, where the metallic compound is dissolved away from the gangue. Each method is matched to a particular class of ore, and the ability to choose the correct method is a direct consequence of understanding the physical and chemical differences between the ore and the gangue. Since concentration removes the bulk of the waste before any fuel or reagent is spent, it is both the cheapest and the most logical first operation in the entire extraction sequence, and it leads directly to the thermal treatments of calcination and roasting that form the next stage of metallurgy.