Subject: Inorganic Chemistry Chapter: Metallurgy Topic: 14.7 Iron and Copper – Study extraction processes of important metals
Iron and copper are two of the most important metals in human history, and their names are linked with whole periods of civilisation, the Iron Age and the Bronze Age. Both metals are extracted from their ores on a vast industrial scale, and their extraction processes illustrate almost every principle of metallurgy that we have studied so far. Iron is a moderately reactive metal obtained by the carbon reduction of its oxide ores in the blast furnace, while copper is a less reactive metal obtained by the self-reduction of its sulphide ore, copper pyrites. Because the two processes use different ores, different furnaces and different chemistry, they make excellent comparative study material.
Iron is the second most abundant metal in the earth's crust, and its most important ores are haematite, Fe2O3, and magnetite, Fe3O4. The extraction of iron is carried out in a tall structure called the blast furnace, in which the ore, coke and limestone are fed from the top and a blast of hot air is forced from the bottom. The coke provides the heat and the reducing agent, the limestone acts as the flux to remove the gangue as slag, and the iron oxide is reduced in stages first to ferrous oxide and then to iron. The product of the blast furnace is called pig iron or cast iron.
Copper is extracted from copper pyrites, CuFeS2, by a process that combines roasting and self-reduction. The ore is concentrated by froth floatation, roasted in a limited supply of air, and then smelted in a reverberatory furnace where the copper sulphide reacts with its own oxide to give copper metal. The impure copper produced is called blister copper, and it is refined electrolytically to give pure copper of 99.9 percent purity. In this chapter we will study the extraction of both metals in detail, including the reactions in the blast furnace and the smelting of copper, and compare the two processes.
The important ores of iron are haematite, Fe2O3, which is the most widely used, magnetite, Fe3O4, limonite, Fe2O3.3H2O, and siderite, FeCO3. Iron pyrites, FeS2, is not used as an ore because it contains sulphur, which makes the iron brittle. The haematite ore used in the blast furnace is usually concentrated by washing and magnetic separation to remove the gangue. The blast furnace is a tall steel tower lined inside with refractory bricks, and it operates continuously, with ore, coke and limestone fed from the top and molten iron and slag tapped from the bottom.
The blast furnace is about 30 metres tall and is kept hot by a blast of preheated air, and sometimes oxygen, that is forced through tuyeres near the bottom. The coke burns in this blast to produce carbon dioxide, which immediately reacts with more coke to form carbon monoxide. The reactions are C plus O2 giving CO2, and CO2 plus C giving 2CO. The carbon monoxide rises through the furnace and acts as the main reducing agent for the iron oxide, while the hot ascending gases heat the descending charge so that all the reactions take place at high temperature.
The four zones of the blast furnace have different temperatures and different reactions. In the upper zone, at about 400 degrees Celsius, the iron oxide is reduced by carbon monoxide. In the middle zone, at about 900 degrees Celsius, limestone decomposes to lime and carbon dioxide, and the lime reacts with the silica of the gangue to form slag of calcium silicate. In the lower and hottest zone, above 1300 degrees Celsius, the iron oxide is reduced directly by carbon and the metal melts. The molten iron and slag collect at the bottom, where they separate into two layers, and they are tapped off through separate holes.
The reduction of iron oxide by carbon monoxide takes place in steps. Haematite, Fe2O3, is first reduced to magnetite, Fe3O4, then to ferrous oxide, FeO, and finally to iron. The three stepwise reductions are represented as 3Fe2O3 plus CO giving 2Fe3O4 plus CO2, Fe3O4 plus CO giving 3FeO plus CO2, and FeO plus CO giving Fe plus CO2. In the hottest part of the furnace, carbon itself directly reduces the iron oxide, as in Fe2O3 plus 3C giving 2Fe plus 3CO. The carbon monoxide is regenerated when carbon dioxide meets more coke, so the reducing atmosphere is maintained throughout the furnace.
The gangue in the iron ore is mainly silica, SiO2, which has a high melting point and would remain mixed with the metal if it were not removed. The limestone flux decomposes to lime, CaO, and the lime combines with the silica to form calcium silicate, CaSiO3, which melts at the furnace temperature and floats on top of the molten iron. This molten calcium silicate is the slag, and the reaction is CaO plus SiO2 giving CaSiO3. The slag protects the molten iron from re-oxidation and is tapped off separately, and it is used for making roads and cement.
The molten iron that collects at the bottom of the furnace is called pig iron, because the sand moulds used to cast it resemble piglets feeding from a sow. Pig iron contains about 4 percent carbon together with silicon, manganese, phosphorus and sulphur, and it is hard but brittle. Pig iron is converted into cast iron by remelting and casting, into wrought iron by removing most of the carbon, and into steel by controlled removal of the carbon and other impurities. The blast furnace therefore produces the raw material for the entire iron and steel industry.
Copper is extracted from its sulphide ore copper pyrites, CuFeS2, through a sequence of concentration, roasting, smelting and refining. The ore is first concentrated by froth floatation, because the sulphide particles are wetted by oil and float with the froth while the gangue settles. The concentrated ore is then roasted in a limited supply of air, during which moisture and sulphur are removed and part of the copper and iron sulphides is converted into oxides. During roasting, cuprous oxide is formed from a part of the copper sulphide, while the iron sulphide is largely oxidised to ferrous oxide.
The roasted ore is then mixed with sand and smelted in a reverberatory furnace. The ferrous oxide reacts with the silica of the sand to form a slag of ferrous silicate, FeSiO3, which floats on the surface, while the remaining copper sulphide and cuprous oxide sink below the slag to form a molten layer called copper matte. The matte is a mixture of cuprous sulphide, Cu2S, and some ferrous sulphide, and it is transferred to a converter for the final reduction. The reactions of roasting and smelting produce sulphur dioxide, which is used in the manufacture of sulphuric acid.
In the converter, air is blown through the molten matte, and the remaining ferrous sulphide is oxidised and removed as slag. The cuprous sulphide then undergoes self-reduction, in which the cuprous sulphide reacts with the cuprous oxide formed by oxidation to give copper metal and sulphur dioxide. The reaction is Cu2S plus 2Cu2O giving 6Cu plus SO2. The copper obtained is called blister copper, because the sulphur dioxide escaping during solidification leaves blowholes on its surface that resemble blisters. Blister copper is about 98 percent pure and contains impurities of iron, sulphur and oxygen.
Blister copper is refined by two methods. The first is furnace refining or poling, in which the blister copper is melted in a reverberatory furnace and a stream of air is passed through it to oxidise the impurities such as iron, sulphur and zinc, which are removed as slag or gases. The molten copper is then stirred with green wooden poles, and the reducing gases released from the wood, mainly carbon monoxide and hydrogen, reduce any cuprous oxide back to copper. This process is called poling, and the copper obtained, called tough pitch copper, is about 99.5 percent pure.
The second and more important method is electrolytic refining, which gives copper of the highest purity for electrical use. In the electrolytic cell, impure copper is made the anode and a thin sheet of pure copper is made the cathode, with a solution of copper sulphate acidified with sulphuric acid as the electrolyte. When current is passed, copper dissolves from the anode and deposits on the cathode in a pure form, while the impurities either go into solution or settle at the bottom as anode mud. The anode mud contains valuable metals such as gold, silver and platinum, which are recovered separately and make the process economically attractive.
The pure electrolytic copper is about 99.9 percent pure and is used for electrical wires, cables and other applications where high conductivity is essential. The entire copper extraction sequence, from froth floatation through roasting, smelting, converting and refining, is a complete illustration of metallurgy because it uses concentration, roasting, self-reduction and electrolytic refining in a single industrial chain. Copper and iron together demonstrate how the same principles of metallurgy are applied differently to metals of different reactivity.
| Feature | Iron | Copper |
|---|---|---|
| Main ore | Haematite Fe2O3 | Copper pyrites CuFeS2 |
| Concentration | Washing, magnetic separation | Froth floatation |
| Type of treatment | Calcination not needed | Roasting and smelting |
| Reducing agent | Carbon monoxide and carbon | Self-reduction of Cu2S |
| Main furnace | Blast furnace | Reverberatory furnace and converter |
| Product before refining | Pig iron | Blister copper |
| Refining | Converted to steel | Electrolytic refining |
| Key by-product | Slag CaSiO3 | SO2 for sulphuric acid |
| Reaction | Process |
|---|---|
| C + O2 gives CO2 | Combustion of coke in blast furnace |
| CO2 + C gives 2CO | Regeneration of carbon monoxide |
| Fe2O3 + 3CO gives 2Fe + 3CO2 | Reduction of haematite by CO |
| CaO + SiO2 gives CaSiO3 | Slag formation in blast furnace |
| 2Cu2S + 3O2 gives 2Cu2O + 2SO2 | Roasting of copper pyrites |
| Cu2S + 2Cu2O gives 6Cu + SO2 | Self-reduction in the converter |
flowchart TD
A[Iron and Copper Extraction] --> B[Iron]
A --> C[Copper]
B --> B1[Ore: haematite Fe2O3]
B --> B2[Blast furnace]
B --> B3[Reduced by CO and C]
B --> B4[Limestone flux - CaO]
B --> B5[Slag: CaSiO3]
B --> B6[Product: pig iron]
B --> B7[Becomes steel by removing carbon]
C --> C1[Ore: copper pyrites CuFeS2]
C --> C2[Froth floatation]
C --> C3[Roasting in limited air]
C --> C4[Smelting to copper matte]
C --> C5[Converter self-reduction]
C --> C6[Cu2S + 2Cu2O gives 6Cu + SO2]
C --> C7[Blister copper]
C --> C8[Electrolytic refining - anode mud has Au, Ag]
A --> D[Both use slag formation and give SO2]
The following diagrams show the construction of the blast furnace for iron extraction and the flow of the copper extraction process.
Iron and copper provide the two classic case studies of metallurgy because their extraction processes are completely different even though they are both based on the same general principles. Iron, a moderately reactive metal, is extracted in the blast furnace by the reduction of haematite with carbon monoxide and carbon, with limestone removing the silica gangue as calcium silicate slag, and the product is pig iron which becomes the raw material for steel. Copper, a less reactive metal, is extracted from copper pyrites through froth floatation, roasting, smelting to copper matte and finally self-reduction in the converter, giving blister copper which is then purified electrolytically to 99.9 percent purity with the recovery of gold and silver from the anode mud. Together the two processes illustrate concentration, roasting, smelting, self-reduction, slag formation and electrolytic refining in a single sweep, and they prepare the student perfectly for the practice questions that follow in the next chapter.